Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 1.8 MPa (264 psi) | 90.0 °C @Thickness 6.40 mm |
194 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Cycolac® X11 ABS Automotive: High heat resistance. Excellent flow/impact balance. UL94 HB rated. High gloss. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 90.0 °C @Thickness 3.20 mm |
194 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Cycoloy® C2950 PC+ABS Non-chlorinated and non-brominated flame retardant PC/ABS offering balanced flow and impact plus improved heat resistance intended for various applications. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 90.0 °C @Thickness 3.20 mm |
194 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Cycoloy® C2950 PC+ABS (Asia Pacific) Non-chlorinated and non-brominated flame retardant PC/ABS offering balanced flow and impact plus improved heat resistance intended for various applications. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 90.0 °C @Thickness 6.40 mm |
194 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Cycoloy® C6200 PC+ABS (Asia Pacific) Non-chlorinated, nombrominated flame retardant PC/ABS offering balanced heat, flow and impact to meet various application needs. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 90.0 °C @Thickness 6.40 mm |
194 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Cycoloy® C6600 PC+ABS Nonbrominated, nonchlorinated FR PC+ABS with balanced flow, impact and hydrolytic stability for a wide variety of applications including business equipment, monitors, enclosures, among others. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 90.0 °C @Thickness 6.40 mm |
194 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Cycoloy® C6600 PC+ABS (Asia Pacific) CYCOLOY C6600 is a FR PC+ABS of nonbrominated, nonchlorinated flame retardant systems with balanced flow, impact and hydrolytic stability for a wide variety of applications including business equipm.. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 90.0 °C @Thickness 6.35 mm |
194 °F @Thickness 0.250 in |
Annealed; ASTM D648 |
PolyOne Geon™ HTX M6230 Polyvinyl Chloride Alloy (PVC Alloy) Information provided by PolyOne |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 90.0 °C @Thickness 6.40 mm |
194 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics Cycoloy® C6200 PC+ABS Non-chlorinated, nombrominated flame retardant PC/ABS offering balanced heat, flow and impact to meet various application needs. |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 90.0 °C @Thickness 6.40 mm |
194 °F @Thickness 0.252 in |
ASTM D648 |
LG Chemical HI121H ABS, High Stiffness Feature: Injection Molding, High StiffnessApplication: Electric & Electronic Products, Miscellaneous GoodsCAS No. 9003-56-9Information provided by LG Chemical |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 90.0 °C @Thickness 6.40 mm |
194 °F @Thickness 0.252 in |
ASTM D648 |
LG Chemical HI153 ABS, High Flow Feature: Injection Molding, High Flow, Good WeatherabilityApplication: Electric & Electronic Products, Miscellaneous GoodsCAS No. 9003-56-9Information provided by LG Chemical |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 90.0 °C @Thickness 6.40 mm |
194 °F @Thickness 0.252 in |
ASTM D648 |
LG Chemical HT700 ABS, High Stiffness Feature: Injection Molding, High StiffnessApplication: Electric & Electronic Products, Miscellaneous GoodsCAS No. 9003-56-9Information provided by LG Chemical |
|||
Deflection Temperature at 1.8 MPa (264 psi) | 90.0 °C @Thickness 3.17 mm |
194 °F @Thickness 0.125 in |
Unannealed; ASTM-D648 |
Ineos ABS Lustran® SMA 2171 SMA, Injection Molding Grade Lustran® SMA 2171 is a high heat injection molding grade of impact-modified SMA (styrene/maleic anhydride) terpolymer offering an exceptional balance of processability and performance. Lustran®.. |