Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 133 °C @Thickness 6.40 mm |
271 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics NORYL NH5020 PPE+PS Noryl* NH5020 Resin is an unreinforced blend of Polyphenylene Ether(PPE) + Polystyrenre resin. The material offers a good balance of heat, flow, hydrolytic stability, and non-halogenated flame reta.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 133 °C @Thickness 6.40 mm |
271 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics NORYL NH5020 PPE+PS (Asia Pacific) Noryl* NH5020 Resin is an unreinforced blend of Polyphenylene Ether(PPE) + Polystyrenre resin. The material offers a good balance of heat, flow, hydrolytic stability, and non-halogenated flame reta.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 133 °C @Thickness 6.40 mm |
271 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics NORYL NH5020 PPE+PS (Europe-Africa-Middle East) Noryl* NH5020 Resin is an unreinforced blend of Polyphenylene Ether(PPE) + Polystyrenre resin. The material offers a good balance of heat, flow, hydrolytic stability, and non-halogenated flame reta.. |