Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 96.0 °C @Thickness 12.7 mm |
205 °F @Thickness 0.500 in |
Unannealed; ASTM-D648 |
Ineos ABS Lustran® 633 ABS, Injection Molding Grade Lustran® ABS 633 is a general-purpose injection molding grade of ABS (Acrylonitrile Butadiene Styrene). It offers a good balance of physical properties, high gloss, and good moldability. Typical .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 96.1 °C @Thickness 6.35 mm |
205 °F @Thickness 0.250 in |
Unannealed; ASTM-D648 |
Ineos ABS Triax® 3050 ABS/Nylon Alloy, Injection Molding Grade (Conditioned) Triax® 3050 resin is an ABS (Acrylonitrile Butadiene Styrene)/Nylon 6 alloy for injection molding. It is a semicrystalline thermoplastic with improved stability to light exposure, excellent proce.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 96.1 °C @Thickness 3.20 mm |
205 °F @Thickness 0.126 in |
Unannealed; ASTM D648 |
Styron Magnum™ 1150 EM Acrylonitrile Butadiene Styrene (ABS) Overview: MAGNUM™ ABS resins are thermoplastic materials which provide an excellent balance to processability, impact resistance and heat resistance as imparted by the various polymer compositions... |