Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | -7.00 - 5.00 °C | 19.4 - 41.0 °F | Average value: -2.00 °C Grade Count:3 |
Overview of materials for Silicone Polyurethane, Polycarbonate Based This property data is a summary of similar materials in the MatWeb database for the category "Silicone Polyurethane, Polycarbonate Based". Each property range of values reported is minimum and maxim.. |