Glass Transition Temp, Tg 145 - 148 °C
293 - 298 °F
Average value: 147 °C Grade Count:3
Overview of materials for Polycarbonate, Optical Grade
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Optical Grade". Each property range of values reported is minimum and maximum values of a..