Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | 55.0 - 132 °C | 131 - 270 °F | Average value: 92.8 °C Grade Count:6 |
Overview of materials for Epoxy, Cast, Metal Filled This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Cast, Aluminum Filled". Each property range of values reported is minimum and maximum values of a.. |