Hexcel® HexPly® M14 248°F (120°C) Curing Epoxy Matrix
HexPly® M14 is a modified epoxy resin which provides good adhesion to honeycomb and foam cores. Its self-extinguishing characteristics meet the fire, smoke, and toxicity requirements of aerospace a..