Polymer Property : Glass Transition Temp, Tg = 78.8 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 26.0 °C
78.8 °F
DSC; ASTM E1356-03
NeXolve Clear Optionox® Polyimide Film/Coating
Highly UV durable with excellent weatherability and stability to ozone.Optinox® films and coatings are highly UV durable and exhibit excellent weathering durability, including very high stability ..
Glass Transition Temp, Tg 26.0 °C
78.8 °F
3M Scotchkote™ 162HB Epoxy Coating
3M Scotchkote Epoxy Coating 163HB has been specifically developed as a 100% solids lining for the internals of pipes, tanks, vessels and other equipment in contact with fresh water, sea water, raw w..
Glass Transition Temp, Tg 26.0 - 500 °C
78.8 - 932 °F
Average value: 340 °C Grade Count:44
Overview of materials for Polyimide, Thermoset Film
This property data is a summary of similar materials in the MatWeb database for the category "Polyimide, Thermoset Film". Each property range of values reported is minimum and maximum values of appr..