Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | -14.0 °C | 6.80 °F | TR10 |
3M Dyneon™ Fluorel™ FX-11818 Fluoroelastomer VF2 + HFP + TFE Terpolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 68.6%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. 68.6% F grade terpolymer for difficul.. |
|||
Glass Transition Temp, Tg | -14.0 °C | 6.80 °F | TR10 |
3M Dyneon™ Fluorel™ FT-2350 Fluoroelastomer VF2 + HFP + TFE Terpolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 68.6%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. Improved retention of elongation afte.. |
|||
Glass Transition Temp, Tg | -14.0 °C | 6.80 °F | TR10 |
3M Dyneon™ Fluorel II™ FX-11900 Fluoroelastomer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Incorporated cure polymer, 59%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, and 4% Ca(OH)2. Excellent processability. Good metal a.. |
|||
Glass Transition Temp, Tg | -14.0 °C | 6.80 °F | TR10 |
3M Dyneon™ Fluorel™ FT-2430 Fluoroelastomer VF2 + HFP + TFE Terpolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Non-incorporated cure polymer, 69%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, 4% Ca(OH)2, 1.4% Dihydroxy Crosslinker, 0.4% Phospho.. |
|||
Glass Transition Temp, Tg | -14.0 °C | 6.80 °F | TR10 |
3M Dyneon™ Fluorel™ FT-2481 Fluoroelastomer VF2 + HFP Dipolymer
(discontinued **) Data provided by the manufacturer, Dyneon LLC.Non-incorporated cure polymer, 68.6%F in polymer with 22% Medium Thermal Carbon Black (N990), 2% MgO, 4% Ca(OH)2, 1.4% Dihydroxy Crosslinker, 0.4% Phosp.. |
|||
Glass Transition Temp, Tg | -14.0 °C | 6.80 °F | |
Mallard Creek Polymers ROVENE® 4150 SBR Latex ROVENE® 4150 is a medium-firm, self-XLing, carboxylated styrene-butadiene (SBR) latex emulsion. Its styrene content (55%) permits its use in formulating carpet and flooring mastics. This versatil.. |
|||
Glass Transition Temp, Tg | -14.0 °C | 6.80 °F | DSC heating rate = -10° C/min |
Kuraray HYBRAR® H7125 Hydrogenated Thermoplastic Rubber Description: HYBRAR® is another in the series of new high performance thermoplastic rubbers developed by KURARAY using their unique isoprene technology. HYBRAR® is a special thermoplastic rubb.. |