Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | 250 °C | 482 °F | DSC; IPC-TM-650.2.4.25c |
Park Electrochemical Nelco® N8000Q Cyanate Ester Epoxy Laminate and Prepreg The Nelco N8000 is a high-Tg cyanate ester laminate and prepreg system that provides superior performance and product integrity and is ideal for board designs with higher layer counts, finer lines a.. |
|||
Glass Transition Temp, Tg | 250 °C | 482 °F | TMA; IPC-TM-650.2.4.24c |
Park Electrochemical Nelco® N7000-1 Polyimide Laminate and Prepreg The Nelco N7000-1 series of polyimide laminate and prepreg has alow Z-axis expansion and high Tg offering PCB manufacturers consistent board performance and reliability. N7000-1 is a good choice for.. |
|||
Glass Transition Temp, Tg | 250 °C | 482 °F | TMA; IPC-TM-650.2.4.24c |
Park Electrochemical Nelco® N7000-2 HT/N7000-3 Toughened Polyimide Laminate and Prepreg The Nelco N7000-2 HT laminate and N7000-3 prepreg are a series of toughened polyimide materials for use in high-reliability multilayers. This combined resin system provides excellent thermal perform.. |
|||
Glass Transition Temp, Tg | 250 °C | 482 °F | DSC; IPC-TM-650.2.4.25c |
Park Electrochemical Nelco® N7000-2 V0 Toughened Polyimide Laminate and Prepreg The Nelco N7000-2 V0 series is a next-generation high-Tg polyimide using a toughened resin chemistry to achieve a UL 94-V0 designation. This advanced material is designed for use in a wide variety o.. |
|||
Glass Transition Temp, Tg | 250 °C | 482 °F | DSC; IPC-TM-650.2.4.25c |
Park Electrochemical Nelco® N8000 Cyanate Ester Epoxy Laminate and Prepreg The Nelco N8000 is a high-Tg cyanate ester laminate and prepreg system that provides superior performance and product integrity and is ideal for board designs with higher layer counts, finer lines a.. |
|||
Glass Transition Temp, Tg | 250 °C | 482 °F | By DSC |
Mitsui AURUM® 450 Thermoplastic Polyimide Resin, Non-filled
(discontinued **) AURUM® is an easy melt, processable and recyclable thermoplastic polyimide resin that provides continuous service temperatures to 465° F in its amorphous state and up to 550° F when annealed to i.. |
|||
Glass Transition Temp, Tg | 250 °C | 482 °F | By DSC |
Mitsui AURUM® JGN3030 Thermoplastic Polyimide Resin, Amorphous
(discontinued **) AURUM® is an easy melt, processable and recyclable thermoplastic polyimide resin that provides continuous service temperatures to 465° F in its amorphous state and up to 550° F when annealed to i.. |
|||
Glass Transition Temp, Tg | 250 °C | 482 °F | By DSC |
Mitsui AURUM® JCL3030 Thermoplastic Polyimide Resin, Amorphous, Wear/Friction Grade
(discontinued **) AURUM® is an easy melt, processable and recyclable thermoplastic polyimide resin that provides continuous service temperatures to 465° F in its amorphous state and up to 550° F when annealed to i.. |
|||
Glass Transition Temp, Tg | 250 °C | 482 °F | DSC |
Mitsui AURUM® JCF3030 Polyimide, Carbon Fiber/PTFE Filled
(discontinued **) AURUM JCF3030 is a high-performance polyimide for precision injection molded components and extruded products. A member of the AURUM family of advanced engineering resins, carbon fiber reinforced AU.. |
|||
Glass Transition Temp, Tg | 250 °C | 482 °F | DSC |
Mitsui AURUM® JCL3030 Polyimide, Carbon Fiber Filled
(discontinued **) AURUM JCL3030 is a high-performance polyimide for precision injection molded components and extruded products. A member of the AURUM family of advanced engineering resins, carbon fiber reinforced AU.. |
|||
Glass Transition Temp, Tg | 250 °C | 482 °F | DSC |
Mitsui AURUM® JCN3030 Polyimide, Carbon Fiber Filled
(discontinued **) AURUM JCN3030 is a high-performance polyimide for precision injection molded components and extruded products. A member of the AURUM family of advanced engineering resins, carbon fiber reinforced AU.. |
|||
Glass Transition Temp, Tg | 250 °C | 482 °F | DSC |
Solvay Specialty Polymers Ajedium™ Film Thermoplastic Polyimide (PI, TP) TPI is a thermoplastic polyimide film that has excellent, thermal, chemical, electrical and physical properties. With a continuous use temperature to 240°C (465°F), TPI films offer superior ra.. |
|||
Glass Transition Temp, Tg | 250 °C | 482 °F | TMA; IPC TM-650 2.4.24 |
Arlon 35N Fast Cure Polyimide Laminate and Prepreg High reliability and high temperature material35N is a pure polyimide laminate and prepreg system for applications requiring high temperature performance. High Tg results in low Z-direction expansi.. |
|||
Glass Transition Temp, Tg | 250 °C | 482 °F | TMA; IPC TM-650 2.4.24 |
Arlon 84N Polyimide Laminate and Prepreg 84N is a high performance ceramic-filled polyimide prepreg based on Arlon's 85N pure polyimide system, designed for use in filling etched areas in polyimide multilayers that contain thick copper lay.. |
|||
Glass Transition Temp, Tg | 250 °C | 482 °F | TMA; IPC TM-650 2.4.24 |
Arlon 85N Polyimide Laminate and Prepreg 85N is a polyimide and laminate prepreg system for PWBs requiring resistance to high temperature, both in process and in end-use application. Bromine-free chemistry provides thermal stability for a.. |
|||
Glass Transition Temp, Tg | 250 °C | 482 °F | TMA; IPC TM-650 2.4.24 |
Arlon 85NT Polyimide Nonwoven Aramid Laminate and Prepreg 85NT is a pure polyimide laminate and prepreg system (Tg = 250°C), reinforced with a non-woven aramid substrate. This system combines the high-reliability features of polyimide (improved PTH relia.. |
|||
Glass Transition Temp, Tg | 250 °C | 482 °F | TMA; IPC TM-650 2.4.24 |
Arlon EP2 Enhanced Polyimide Laminate and Prepreg High reliability and high temperature materialEP2 Enhanced Polyimide is the next generation of polyimide and prepreg products, engineered for improved properties and processing and for applications .. |
|||
Glass Transition Temp, Tg | 250 °C | 482 °F | TMA; IPC TM-650 2.4.24 |
Arlon 33N Polyimide Laminate and Prepreg High reliability and high temperature material33N is a flame retardant polyimide laminate and prepreg system where the excellent high performance properties of polyimide need to be combined with fla.. |
|||
Glass Transition Temp, Tg | 250 °C | 482 °F | DSC |
Mitsui AURUM® JGN3030 Polyimide, Glass Fiber Filled
(discontinued **) AURUM JGN3030 is a high performance thermoplastic polyimide for precision injection molded components and extruded products. A member of the AURUM family of advanced engineering resins, glass fiber .. |
|||
Glass Transition Temp, Tg | 250 °C | 482 °F | DSC |
Mitsui AURUM® PL450C Polyimide
(discontinued **) AURUM PL450C is a high performance thermoplastic polyimide for precision injection molded components and extruded products. A member of the AURUM family of advanced engineering resins, unfilled AURU.. |