Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | 230 °C | 446 °F | Laminate; post cure |
Park Electrochemical Nelcote® E-720 Epoxy Prepreg, 581 Quartz Reinforced Nelcote® E-720 is a modified epoxy resin system designed to retain excellent mechanical properties after extended exposure to high temperature. E-720 has a proven history in many demanding aerospac.. |
|||
Glass Transition Temp, Tg | 230 °C | 446 °F | Laminate; post cure |
Park Electrochemical Nelcote® E-720 Epoxy Prepreg, 7781 E-Glass Reinforced Nelcote® E-720 is a modified epoxy resin system designed to retain excellent mechanical properties after extended exposure to high temperature. E-720 has a proven history in many demanding aerospac.. |
|||
Glass Transition Temp, Tg | 230 °C | 446 °F | Laminate; post cure |
Park Electrochemical Nelcote® E-746 Epoxy Prepreg, 3k 5HS Carbon Reinforced Nelcote® E-746 is a modified epoxy resin system designed to retain excellent mechanical properties after extended exposure to high temperature. E-746 has a proven history in many demanding aerospac.. |
|||
Glass Transition Temp, Tg | 230 °C | 446 °F | Laminate; post cure |
Park Electrochemical Nelcote® E-746 Epoxy Prepreg, 581 Quartz Reinforced Nelcote® E-746 is a modified epoxy resin system designed to retain excellent mechanical properties after extended exposure to high temperature. E-746 has a proven history in many demanding aerospac.. |
|||
Glass Transition Temp, Tg | 230 °C | 446 °F | Laminate; post cure |
Park Electrochemical Nelcote® E-746 Epoxy Prepreg, 7781 E-Glass Reinforced Nelcote® E-746 is a modified epoxy resin system designed to retain excellent mechanical properties after extended exposure to high temperature. E-746 has a proven history in many demanding aerospac.. |
|||
Glass Transition Temp, Tg | 230 °C | 446 °F | DMA (SSYS) |
RedEye On Demand Polyphenylsulfone (PPSF), Rapid Prototyping Material Polyphenylsulfone (PPSF) is a durable high-end thermoplastic that can be used in the toughest applications. Parts built in PPSF can handle heat near 400°F (204°C), it resists petroleum products, a.. |
|||
Glass Transition Temp, Tg | 230 °C | 446 °F | DMA (SSYS) |
Stratasys® Polyphenylsulfone PPSF/PPSU (polyphenylsulfone) material has the greatest strength, heat and chemical resistance of all Stratasys materials - ideal for aerospace, automotive and medical applications. Stratasys FDM (F.. |
|||
Glass Transition Temp, Tg | 230 °C | 446 °F | DAM (SSYS) |
Proto3000 PPSF Fused Deposition Modeling Polymer Description: PPSF/PPSU (polyphenylsulfone) material has the greatest heat and chemical resistance of all Fortus materials - ideal for aerospace, automotive and medical applications. PPSF parts manuf.. |