Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | 215.5 °C | 419.9 °F | ASTM D3418 |
Westlake Plastics Tempalux® Film Made from ULTEM® Polyetherimide Resin High heat deflection and continuous use temperature. Inherent flame resistance. Extremely low NBS smoke evolution & superior limiting oxygen index.Ultem® is a trade name of GE Plastics. Informat.. |