Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | 189 °C | 372 °F | |
Bulk Molding Compounds BMC 940 Vinyl Ester Bipolar Plate Material Product Introduction: Bulk Molding Compounds, Inc. is the largest manufacturer of thermoset bulk molding compounds in North America, serving the automotive, appliance, and electrical markets. BMC t.. |