Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | 145 °C | 293 °F | ASTM D3418 |
Quadrant EPP Quadrant PC 1000 Extruded, Unfilled, Polycarbonate (ASTM Product Data Sheet) |
|||
Glass Transition Temp, Tg | 145 - 150 °C | 293 - 302 °F | Average value: 148 °C Grade Count:5 |
Overview of materials for Polycarbonate/Styrenic Alloy This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Styrenic Alloy". Each property range of values reported is minimum and maximum values of a.. |
|||
Glass Transition Temp, Tg | 145 °C | 293 °F | |
Cookson Group Plaskon® 2929BNSC Epoxy Molding Compound
(discontinued **) Test specimens were transfer molded and post cured 4 hours at 175°C.An epoxy molding compound for the encapsulation of semiconductor devices and fiber optics. Excellent moldability (good release, .. |
|||
Glass Transition Temp, Tg | 145 °C | 293 °F | |
Cookson Group Plaskon® 3400F Epoxy Molding Compound
(discontinued **) Test specimens were transfer molded and post cured 4 hours at 175°C.A fast curing, reduced-stress epoxy molding compound for the encapsulation of semiconductor devices including DIPs, PLCCs, SOICs .. |
|||
Glass Transition Temp, Tg | 145 - 155 °C | 293 - 311 °F | DMA |
Hexcel® HexPly® 1458 160°C-180°C Curing Epoxy Matrix HexPly® 1458 is a self-extinguishing and self-adhesive modified epoxy resin system for monolithic and sandwich structures. HexPly® 1458 has excellent temperature and moisture resistance. It has a .. |
|||
Glass Transition Temp, Tg | 145 °C | 293 °F | DMTA |
Hexcel® HexPly® 916 120°C Curing Epoxy Matrix HexPly® 916 is a self-extinguishing modified epoxy matrix system with very high self adhesive properties. It is an ideal system for single shot honeycomb sandwich manufacture, with good drape chara.. |
|||
Glass Transition Temp, Tg | 145 °C | 293 °F | Plain Cast Resin; ASTM D3418 |
TSE Industries EcoWIND® P200G High Performance Filament Winding Polyurethane Resin for Pipes TSE-EcoWIND® resins are “Environmentally-Preferred Products” or EPP’s. They are a pair of polyurethane resins free of Styrene, and are “ultra-low” emitting during application. TSE-EcoWIND® re.. |
|||
Glass Transition Temp, Tg | 145 °C | 293 °F | |
Covestro Makrolon® 2205 Polycarbonate, Injection Grade Exceptionally good flow injection molding grade with easy mold release, for parts with a low wall thickness and long flow paths.Information provided by Bayer.As of 1 September 2015, Bayer MaterialSc.. |
|||
Glass Transition Temp, Tg | 145 °C | 293 °F | 10°C/min; ISO 11357-1,-2 |
Covestro Makrolon® 2256 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Food contact quality•.. |
|||
Glass Transition Temp, Tg | 145 °C | 293 °F | 10°C/min; ISO 11357-1,-2 |
Covestro Makrolon® 2258 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Medical devices - bioc.. |
|||
Glass Transition Temp, Tg | 145 °C | 293 °F | 10°C/min; ISO 11357-1,-2 |
Covestro Makrolon® 2405 MAS048 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Low.. |
|||
Glass Transition Temp, Tg | 145 °C | 293 °F | ISO 11357-1/-2 |
Covestro Makrolon® 2556 Polycarbonate MVR (300 °C/1.2 kg) 14 cm3/10 minEasy releaseGood hydrolysis resistanceInjection moldingAvailable in transparentTranslucent and opaque colorsFood contact gradePreprocessingMax. Water content |
|||
Glass Transition Temp, Tg | 145 °C | 293 °F | ISO 11357-1/-2 |
Covestro Makrolon® 2558 Polycarbonate ISO 7391-PC,MR,(,,)-18-9MVR (300 °C/1.2 kg) 14.5 cm3/10 minMedical devicessuitable for ETO and steam sterilization at 121 °CComplies with the requirements of FDA-modified ISO 10993-1 and USP Class.. |
|||
Glass Transition Temp, Tg | 145 °C | 293 °F | ISO 11357-1/-2 |
Covestro Makrolon® 2656 Polycarbonate ISO 7391-PC,MR,(,,)-18-9Global gradeMVR (300 °C/1.2 kg) 12.5 cm3/10 minFood contact qualityMedium viscosityEasy releaseGood hydrolysis resistanceInjection molding - Melt temperature 280 - 320 °CAv.. |
|||
Glass Transition Temp, Tg | 145 °C | 293 °F | ISO 11357-1/-2 |
Covestro Makrolon® 2665 Polycarbonate, Flame Retardant Grade ISO 7391-PC,MFR,(,,)-18-9Global gradeMVR (300 °C/1.2 kg) 12.5 cm3/10 minChlorine- and bromine-free flame retardantUL 94V-2/1.5 mm and 3.0 mmMedium viscosityEasy releaseInjection molding - Melt temp.. |
|||
Glass Transition Temp, Tg | 145 °C | 293 °F | ISO 11357-1/-2 |
Covestro Makrolon® 2865 Polycarbonate, Flame Retardant Grade ISO 7391-PC,MFR,(,,)-09-9Global gradeMVR (300 °C/1.2 kg) 9.5 cm3/10 minChlorine- and bromine-free flame retardantUL 94V-2/1.5 mm and 3.0 mmMedium viscosityEasy releaseInjection molding - Melt tempe.. |
|||
Glass Transition Temp, Tg | 145 °C | 293 °F | 10°C/min; ISO 11357-1,-2 |
Covestro Makrolon® 3107 MAS167 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Hig.. |
|||
Glass Transition Temp, Tg | 145 °C | 293 °F | 10°C/min; ISO 11357-1,-2 |
Covestro Makrolon® FU4007 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Furniture applications.. |
|||
Glass Transition Temp, Tg | 145 °C | 293 °F | ISO 11357-1/-2 |
Covestro Makrolon® OD2015 Polycarbonate Global gradeOptical storage mediaLow viscosityEasy releaseHigh purityInjection moldingAvailable in natural color onlyPreprocessingMax. Water content |
|||
Glass Transition Temp, Tg | 145 - 150 °C | 293 - 302 °F | |
A. Schulman ComAlloy Comtuf® 410 Polycarbonate/Polyester Alloy Data provided by the manufacturer, ComAlloy International Company. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been integrated into the A Sc.. |
|||
Glass Transition Temp, Tg | 145 - 150 °C | 293 - 302 °F | |
A. Schulman ComAlloy Comtuf® 520 Polycarbonate/Styrenic Alloy Data provided by the manufacturer, ComAlloy International Company. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been integrated into the A Sc.. |
|||
Glass Transition Temp, Tg | 145 - 150 °C | 293 - 302 °F | |
A. Schulman ComAlloy Comtuf® 523 Polycarbonate/Styrenic Alloy Data provided by the manufacturer, ComAlloy International Company. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been integrated into the A Sc.. |
|||
Glass Transition Temp, Tg | 145 - 150 °C | 293 - 302 °F | |
A. Schulman ComAlloy Hiloy® 511 Polycarbonate, Glass Reinforced, UL Data provided by the manufacturer, ComAlloy International Company.10% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Glass Transition Temp, Tg | 145 - 150 °C | 293 - 302 °F | |
A. Schulman ComAlloy Hiloy® 513 Polycarbonate, Glass Reinforced, UL Data provided by the manufacturer, ComAlloy International Company.30% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Glass Transition Temp, Tg | 145 - 150 °C | 293 - 302 °F | |
A. Schulman ComAlloy Hiloy® 514 Polycarbonate, Glass Reinforced, UL Data provided by the manufacturer, ComAlloy International Company.40% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Glass Transition Temp, Tg | 145 - 150 °C | 293 - 302 °F | |
A. Schulman ComAlloy Hiloy® 517 Polycarbonate, Carbon Fiber Reinforced Data provided by the manufacturer, ComAlloy International Company.30% Carbon Fiber Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Glass Transition Temp, Tg | 145 - 150 °C | 293 - 302 °F | |
A. Schulman ComAlloy Lubrilon® 512 Polycarbonate, Glass Fiber/PTFE, UL Data provided by the manufacturer, ComAlloy International Company. High performance and excellent lubricity with minimal surface wear.The ComAlloy product line has been integrated into the A Schulma.. |
|||
Glass Transition Temp, Tg | 145 °C | 293 °F | ISO 11357-1/-2 |
Covestro Makrolon® LED2245 Polycarbonate ISO 7391-PC,MRT,(,,)-24-9Global gradeFormerly Makrolon DP1-1857MVR (300 °C/1.2 kg) 36 cm3/10 minLight guidesPC with highest transmissionLow viscosityEasy releaseInjection molding - Melt temperature.. |
|||
Glass Transition Temp, Tg | 145 °C | 293 °F | ASTM D3418 |
Quadrant EPP Quadrant LSG PC (ASTM Product Data Sheet) Data provided by Quadrant Engineering Plastic Products. |
|||
Glass Transition Temp, Tg | 145 °C | 293 °F | Plain Cast Resin; ASTM D3418 |
TSE Industries EcoWIND® P200G High Performance Filament Winding Polyurethane Resin for Pipes TSE-EcoWIND® resins are “Environmentally-Preferred Products” or EPP’s. They are a pair of polyurethane resins free of Styrene, and are “ultra-low” emitting during application. TSE-EcoWIND® re.. |