Polymer Property : Glass Transition Temp, Tg = 277 °F
Polymer Property :
Glass Transition Temp, Tg =
277 °F
Product List
Thermal Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties
Metric
English
Comments
Glass Transition Temp, Tg
136
°C
277
°F
DSC
Zeon Chemicals Zeonex® 690R Cyclo-Olefin Polymer
Glass Transition Temp, Tg
136
°C
277
°F
Zeon Chemicals Zeonex® RS420 Cyclo-Olefin Polymer