Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | -9.00 °C | 15.8 °F | |
Styron XZ 92069.01 Carboxylated SB Performance Features: Excellent crack bridging, APEO-freeApplications: Waterproofing MembranesAsia PacificInformation provided by Styron |
|||
Glass Transition Temp, Tg | -9.00 °C | 15.8 °F | |
Styron XZ 92069.01 Carboxylated SB Performance Features: APEO free, excellent crack bridgingApplications: Waterproofing MembranesEuropeInformation provided by Styron |
|||
Glass Transition Temp, Tg | -9.00 °C | 15.8 °F | |
Styron XZ 92069.01 SB Latex Performance Features: Excellent crack bridging, APEO-freeApplications: Waterproofing MembranesLatin America/South AmericaInformation provided by Styron |
|||
Glass Transition Temp, Tg | -9.00 °C | 15.8 °F | |
Styron XZ 92087.00 Carboxylated SB Performance Features: Anionic bitumen compatible, APEO-freeApplications: Waterproofing MembranesAsia PacificInformation provided by Styron |
|||
Glass Transition Temp, Tg | -9.00 °C | 15.8 °F | |
Styron XZ 92087.00 Carboxylated SB Performance Features: APEO free, anionic bitumen compatibleApplications: Waterproofing MembranesEuropeInformation provided by Styron |