Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | 61.0 °C | 142 °F | DSC, both heating and cooling speeds of 20°C/min |
Noltex Soarnol® ST110 Ethylene Vinyl Alcohol Copolymer Modified DC3203; improved flex crack resistance and thermoformability. Ethylene content 32 mol%. Volatile matter 0.3%.The gas barrier property of Soarnol is about forty times better than that of n.. |
|||
Glass Transition Temp, Tg | 61.0 °C | 142 °F | TM R050-25 |
Resinlab® EP965 Clear Unfilled Electronic Grade Epoxy Encapsulant Resinlab™ EP965 Clear is a two part unfilled electronic grade epoxy encapsulant designed for medium sized castings. It cures at room temperature to a tough, semi-rigid polymer. It has good wetting .. |
|||
Glass Transition Temp, Tg | 61.0 °C | 142 °F | DSC, both heating and cooling speeds of 20°C/min |
Noltex Soarnol® DC3212 Ethylene Vinyl Alcohol Copolymer Ethylene content 32 mol%. Volatile matter 0.3%.The gas barrier property of Soarnol is about forty times better than that of nylon, therefore, Soarnol allows design of lower cost packages by using a.. |
|||
Glass Transition Temp, Tg | 61.0 °C | 142 °F | |
Armstrong A-34 Epoxy Adhesive This white paste material is a fast-curing adhesive with a working life of 20-25 minutes in a 100-gram mass. Mixing ratio is a convenient 1:1. A-34 has excellent wetting properties and is suggeste.. |
|||
Glass Transition Temp, Tg | 61.0 °C | 142 °F | TM R050-25 |
Resinlab® EP965 Black Unfilled Electronic Grade Epoxy Encapsulant Resinlab™ EP965 Black is a two part unfilled electronic grade epoxy encapsulant designed for medium sized castings. It cures at room temperature to a tough, semi-rigid polymer. It has good wetting .. |