Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | 52.0 - 58.0 °C | 126 - 136 °F | ASTM D3417 |
NatureWorks® Ingeo™ 4060D Sealant Grade PLA PLA (polylactide) polymer 4060D can be coextruded with other PLA resin to form a sealant layer for biaxially oriented PLA film. This resin has excellent heat seal and hot tack performance with a sea.. |
|||
Glass Transition Temp, Tg | 52.0 - 54.0 °C | 126 - 129 °F | DMA, E |
Proto3000 Objet VeroBlack FullCure870 Rigid Opaque Prototyping Polymer Objet’s FullCure® Materials family of proprietary acrylic-based photopolymer materials enables Objet users to create highly accurate, finely detailed 3D models and parts for a wide range of Rapid .. |
|||
Glass Transition Temp, Tg | 52.0 - 54.0 °C | 126 - 129 °F | DMA, E |
Proto3000 Objet VeroClear FullCure810 Information provided by Proto3000 for their protoyping engineering services. |
|||
Glass Transition Temp, Tg | 52.0 - 54.0 °C | 126 - 129 °F | DMA, E |
Proto3000 Objet VeroGray FullCure850 Rigid Opaque Prototyping Polymer Objet’s FullCure® Materials family of proprietary acrylic-based photopolymer materials enables Objet users to create highly accurate, finely detailed 3D models and parts for a wide range of Rapid .. |
|||
Glass Transition Temp, Tg | 52.0 °C | 126 °F | |
Unitika elitel UE3350 Polyester, Flake Low molecular weight type UE3210, High OH typeUNITIKA l resins are thermoplastic saturated copolymeric polyester resins. l resins are expanding their applications from products such as adhesives, p.. |
|||
Glass Transition Temp, Tg | 52.0 °C | 126 °F | Ultimate Tg; DSC |
Tra-Con Tra-Bond 516H03 Blush-Free Epoxy Adhesive TRA-BOND 516H03 is a modified version of F114 yielding a higher viscosity and lower coefficient of thermal expansion. Information provided by Tra-Con Inc. |
|||
Glass Transition Temp, Tg | 52.0 °C | 126 °F | Ultimate Tg, 24 hrs @ 25°C |
Tra-Con Tra-Duct 2902 Room Temperature Conductive Silver Epoxy Adhesive TRA-DUCT 2902 is an electrically conducting silver-filled epoxy compound recommended for electronic bonding and sealing applications that require a combination of good mechanical and electrical prop.. |
|||
Glass Transition Temp, Tg | 52.0 °C | 126 °F | ETM 300-90 |
ExxonMobil ESCOREZ™ 5400 Petroleum Hydrocarbon Resin Light colored cycloaliphatic hydrocarbon resin. They are designed to tackify a variety of adhesive polymers including EVA, SIS and SEBS block copolymers, natural rubber, synthetic polyisoprene, poly.. |
|||
Glass Transition Temp, Tg | 52.0 °C | 126 °F | ETM 300-90 |
ExxonMobil ESCOREZ™ 5600 Petroleum Hydrocarbon Resin Light colored aromatic modified, cycloaliphatic hydrocarbon resin. Designed to tackify a variety of adhesive polymers including EVA, SIS and SEBS block copolymers and metallocene polyolefines. Avail.. |
|||
Glass Transition Temp, Tg | 52.0 °C | 126 °F | DMA, E" |
3D Systems Accura® Xtreme Plastic for SLA® Systems For use with solid-state stereolithography (SLA®) systemsApplicationsForm, fit and function prototypesDurable AssembliesSnap fit assembliesTough enclosuresConsumer electronic componentsMaster patte.. |
|||
Glass Transition Temp, Tg | 52.0 °C | 126 °F | DMA, E" |
3D Systems Accura® Xtreme White 200 Plastic Ultra tough white plastic to replace CNC Machined polypropylene and ABS articles FeaturesExceptionally tough and durableUsed for challenging functional assembliesUsed for snap fit assembl.. |
|||
Glass Transition Temp, Tg | 52.0 °C | 126 °F | |
3M Scotch-Weld™ 2158 B/A Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive 2158 B/A is a gray, two-part, high strength adhesive that chemically cures at room temperature. It has good adhesion to a variety of substrates including metals, ma.. |
|||
Glass Transition Temp, Tg | 52.0 - 54.0 °C | 126 - 129 °F | DMA, E |
Proto3000 Objet VeroWhitePlus FullCure835 Rigid Opaque Prototyping Polymer Information provided by Proto3000 for their protoyping engineering services. |