Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | 42.0 °C | 108 °F | |
Resinlab® EP1112 Clear Electronic Grade Epoxy Encapsulant Resinlab™ EP 1112 Clear is a two part unfilled fast curing electronic grade epoxy encapsulant designed for small to medium sized castings. It cures completely at room temperature to a tough, flexib.. |
|||
Glass Transition Temp, Tg | 42.0 - 115 °C | 108 - 239 °F | Average value: 73.8 °C Grade Count:6 |
Overview of materials for Epoxy Adhesive, Flexible This property data is a summary of similar materials in the MatWeb database for the category "Epoxy Adhesive, Flexible". Each property range of values reported is minimum and maximum values of appro.. |
|||
Glass Transition Temp, Tg | 42.0 °C | 108 °F | |
Styron DL 275NA Carboxylated SB Performance Features: Strength modifier, heat sealableApplications: Heat SealableNorth AmericaInformation provided by Styron |
|||
Glass Transition Temp, Tg | 42.0 °C | 108 °F | |
Styron DL 275NA Carboxylated SB Performance Features: Strength modifier, reduced blockingApplications: Sound DampeningNorth AmericaInformation provided by Styron |
|||
Glass Transition Temp, Tg | 42.0 °C | 108 °F | |
Unitika elitel UE3620 Polyester, Pellet High elongation type UE3215UNITIKA l resins are thermoplastic saturated copolymeric polyester resins. l resins are expanding their applications from products such as adhesives, paints, ink binders,.. |
|||
Glass Transition Temp, Tg | 42.0 - 46.0 °C | 108 - 115 °F | ASTM E1545-00 |
DSM Somos® WaterClear® Ultra 10122 Optically Clear, Colorless, Rigid, Stereolithography Resin DescriptionDSM Somos® WaterClear Ultra 10122 is a next generation optically clear resin with ABS like properties and good temperature resistance. It produces colorless, functional, accurate parts .. |
|||
Glass Transition Temp, Tg | 42.0 °C | 108 °F | |
Armstrong C-7/W Epoxy Adhesive, 2:3 Mix Ratio A clear, unfilled, medium viscosity adhesive recommended for use with any Armstrong Activator. Physical property data included covers C-7 used with Activators W and H-20. All other Activators may .. |
|||
Glass Transition Temp, Tg | 42.0 °C | 108 °F | |
Resinlab® EP1112 Black Electronic Grade Epoxy Encapsulant Resinlab™ EP 1112 Black is a two part unfilled fast curing electronic grade epoxy encapsulant designed for small to medium sized castings. It cures completely at room temperature to a tough, flexib.. |