Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | -22.2 °C | -8.00 °F | DSC, 10ºC/min; DIN 51.007 |
Lubrizol Advanced Materials PEARLCOAT® 126K Thermoplastic Polyurethane Elastomer
(discontinued **) PEARLCOAT® 126K is a polyester-based TPU, supplied in form of translucent, colorless pellets, combining hardness with excellent low temperature flexibility and medium softening point. PEARLCOAT® 1.. |
|||
Glass Transition Temp, Tg | -22.2 °C | -8.00 °F | ASTM D1329 |
Seals Eastern 7265D Fluorocarbon-Elastomer Formulated Viton-ETP®. High temperature service in aggressive chemicals; Good base resistance.Information provided by Seals Eastern, Inc. |