Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | -52.0 °C | -61.6 °F | |
Teknor Apex TEKRON® 4300-D90B Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
Glass Transition Temp, Tg | -52.0 °C | -61.6 °F | DSC |
Lubrizol Estane® 58070 Thermoplastic Polyurethane Features: Outstanding resiliency, fuel resistance and low temperature flexibility.Uses: Hose and Tube, Injection Molding, Fabric Coating and Wire/CableAvailable in Americas, Europe, Middle East, Afr.. |
|||
Glass Transition Temp, Tg | -52.0 °C | -61.6 °F | DSC |
Lubrizol ESTANE® 58881 Ether Based Thermoplastic Polyurethane Features: Very high tensile strength, excellent low temperature flexibility, and superior abrasion and cut resistanceUses: Extrusion – Wire and cable, Hose and tube & General purposeAvailable in Am.. |
|||
Glass Transition Temp, Tg | -52.0 °C | -61.6 °F | ExxonMobil Method |
ExxonMobil Exact™ 9361 Ethylene-based Plastomer Resin Product Description: Exact 9361 plastomer is an ethylene butene copolymer produced using ExxonMobil Chemical's EXXPOL™ Technology, exhibiting both plastic and elastomeric properties.Key Features:P.. |
|||
Glass Transition Temp, Tg | -52.0 °C | -61.6 °F | DSC, 10°C/min (inf); DuPont Test |
Dow Engage® ENR 7380.00 Ethylene-Butene Copolymer Description: ENR 7380.00 is a revolutionary new ethylene-butene copolymer with higher molecular weight, better toughness, and higher melt strength than other commercially available polyolefin elasto.. |