Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | -40.0 °C | -40.0 °F | ASTM D4065 |
Solvay Specialty Polymers Solef® 1015 Polyvinylidene Fluoride (PVDF)
(Unverified Data**) Solef® 1015 PVDF homopolymer has very high viscosity, suitable for membrane manufacturing. It is available exclusively as powder.Information provided by Solvay Specialty Polymers. |
|||
Glass Transition Temp, Tg | -40.0 °C | -40.0 °F | ASTM D4065 |
Solvay Specialty Polymers Solef® 6008 Polyvinylidene Fluoride (PVDF)
(Unverified Data**) Solef® 6008 PVDF homopolymer is a low-viscosity PVDF resin and is typically processed by injection molding.Information provided by Solvay Specialty Polymers. |
|||
Glass Transition Temp, Tg | -40.0 °C | -40.0 °F | TMA |
Lord Adhesives Thermosetâ„¢ MS-330 Silicone Board Level Encapsulant LORD Thermosetâ„¢ MS-330 encapsulant is a one component silicone specifically designed for use on high-frequency devices including Bluetooth applications. This silicone encapsulant offers excelle.. |
|||
Glass Transition Temp, Tg | -40.0 °C | -40.0 °F | DSC, 10ºC/min; DIN 51.007 |
Lubrizol Advanced Materials PEARLTHANE® 11T85UV Thermoplastic Polyurethane Elastomer PEARLTHANE® 11T85UV is a UV resistant polycaprolactone copolyester based TPU, supplied in form of translucent, colourless or slightly yellowish pellets, featuring adequate hardness with excellent.. |
|||
Glass Transition Temp, Tg | -40.0 °C | -40.0 °F | DSC, 50°F/min; DIN 51.007 |
Lubrizol Advanced Materials Pearlthane® 12T92E Thermoplastic Polyurethane Elastomer PEARLTHANE® 12T92E is a special polyester-based TPU, supplied in form of translucent, colorless pellets, combining hardness with excellent processability and low temperature performance. This gra.. |
|||
Glass Transition Temp, Tg | -40.0 °C | -40.0 °F | ASTM D1329 |
Seals Eastern 5242 Neoprene / Chloroprene General purpose neopreneInformation provided by Seals Eastern, Inc. |
|||
Glass Transition Temp, Tg | -40.0 °C | -40.0 °F | ASTM D1329 |
Seals Eastern 7065 Neoprene / Chloroprene General purpose neopreneInformation provided by Seals Eastern, Inc. |
|||
Glass Transition Temp, Tg | -40.0 °C | -40.0 °F | ASTM E1356 |
Solvay Specialty Polymers Ajedium™ PVDF 9009 Polyvinylidene Fluoride (PVDF) Solef® 9009 PVDF homopolymer is a semi-crystalline fluoropolymer. Solef® film is chemically inert to most acids, aliphatic and aromatic organic compounds, chlorinated solvents and alcohols.Fea.. |
|||
Glass Transition Temp, Tg | -40.0 °C | -40.0 °F | ASTM E1356 |
Solvay Specialty Polymers Solef® 1015 Polyvinylidene Fluoride (PVDF) Solef® 1015 PVDF homopolymer has very high viscosity, suitable for membrane manufacturing. It is available exclusively as powder.Features: Homopolymer; Ultra High ViscosityUses: MembranesAddition.. |
|||
Glass Transition Temp, Tg | -40.0 °C | -40.0 °F | ASTM E1356 |
Solvay Specialty Polymers Solef® 6008 Polyvinylidene Fluoride (PVDF) Solef® 6008 PVDF homopolymer is a low-viscosity PVDF resin and is typically processed by injection molding.Features: Homopolymer; Low ViscosityAdditional Properties: Crystallization Heat - ASTM D.. |
|||
Glass Transition Temp, Tg | -40.0 °C | -40.0 °F | ASTM E1356 |
Solvay Specialty Polymers Solef® 6020 Polyvinylidene Fluoride (PVDF) Solef® 6020 PVDF homopolymer has very high viscosity for membranes and lithium batteries. It is available exclusively as powder.Features: Homopolymer; Ultra High ViscosityUses: Batteries; Membran.. |
|||
Glass Transition Temp, Tg | -40.0 °C | -40.0 °F | ASTM E1356 |
Solvay Specialty Polymers Solef® 60512 Polyvinylidene Fluoride (PVDF) Solef® 60512 PVDF copolymer has high viscosity of the melt and it is a grade for offshore piping.Features: Copolymer; High ViscosityUses: PipingAdditional Properties: Crystallization Heat - ASTM .. |
|||
Glass Transition Temp, Tg | -40.0 - -30.0 °C | -40.0 - -22.0 °F | |
Zeus PVDF Tubing PVDF, polyvinylidene fluoride, delivers high performance at a competitive cost. Its inherent purity positions it as ideal for a variety of applications which involve extreme conditions. PVDF is char.. |
|||
Glass Transition Temp, Tg | -40.0 °C | -40.0 °F | DSC |
Lubrizol Estane® 58144 Thermoplastic Polyurethane Type: Estane® 58144 is a 65D Polyether-type thermoplastic polyurethane (TPU) compound.Features: FDA (contact Lubrizol for details). Pre-drying: 2 hours at 104C (220F) in Dehumidifying Hopper Dryer.. |
|||
Glass Transition Temp, Tg | -40.0 °C | -40.0 °F | 10°C/min |
Covestro Texin® 945U Urethane Thermoplastic Elastomer Key Features:UnfilledU.V. stabilized or stable to weatherSuitable processing methods:Injection moldingProfile extrusionSheet extrusionInformation provided by Bayer Polymers.As of 1 September 2015, B.. |
|||
Glass Transition Temp, Tg | -40.0 - -38.0 °C @Frequency 1.00 Hz |
-40.0 - -36.4 °F @Frequency 1.00 Hz |
DMA |
Arkema Group KYNAR FLEX® 2850-02 Polyvinylidene Fluoride Copolymer - Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani.. |
|||
Glass Transition Temp, Tg | -40.0 - -38.0 °C @Frequency 1.00 Hz |
-40.0 - -36.4 °F @Frequency 1.00 Hz |
DMA |
Arkema Group KYNAR FLEX® 2850-04 Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani.. |
|||
Glass Transition Temp, Tg | -40.0 - -38.0 °C @Frequency 1.00 Hz |
-40.0 - -36.4 °F @Frequency 1.00 Hz |
DMA |
Arkema Group KYNAR® 370 Polyvinylidene Fluoride (PVDF) Homopolymer - Injection Molding Characteristics: Natural resin - translucent, off-white hemispheres. Low melt shrinkage, graphite powder filled. High stability in harsh thermal, chemical and ultraviolet environments. High toug.. |
|||
Glass Transition Temp, Tg | -40.0 - -38.0 °C @Frequency 1.00 Hz |
-40.0 - -36.4 °F @Frequency 1.00 Hz |
DMA |
Arkema Group KYNAR® 740 Black/Red Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion Characteristics: Pigmented. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeability, abrasion resistance; high purityAppli.. |
|||
Glass Transition Temp, Tg | -40.0 - -38.0 °C @Frequency 1.00 Hz |
-40.0 - -36.4 °F @Frequency 1.00 Hz |
DMA |
Arkema Group KYNAR® 740 Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili.. |
|||
Glass Transition Temp, Tg | -40.0 - -38.0 °C @Frequency 1.00 Hz |
-40.0 - -36.4 °F @Frequency 1.00 Hz |
DMA |
Arkema Group KYNAR® 460 Polyvinylidene Fluoride Homopolymer - Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. Broad molecular weight distribution. High stability in harsh thermal, chemical and ultraviolet environments. High toughness a.. |
|||
Glass Transition Temp, Tg | -40.0 - -38.0 °C @Frequency 1.00 Hz |
-40.0 - -36.4 °F @Frequency 1.00 Hz |
DMA |
Arkema Group KYNAR® 720, 720 HDP Polyvinylidene Fluoride Homopolymer- Injection Molding and Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. HDP indicates higher color stability. High stability in harsh thermal, chemical and ultraviolet environments. High toughness .. |
|||
Glass Transition Temp, Tg | -40.0 °C | -40.0 °F | ASTM D4065 |
Solvay Specialty Polymers Solef® 21510 Polyvinylidene Fluoride (PVDF)
(Unverified Data**) Solef® 21510 PVDF copolymer has low viscosity and is suitable for solution processing in lithium batteries applications.Information provided by Solvay Specialty Polymers. |
|||
Glass Transition Temp, Tg | -40.0 °C | -40.0 °F | ASTM D4065 |
Solvay Specialty Polymers Solef® 9009 Polyvinylidene Fluoride (PVDF)
(discontinued **) Solef® 9009 PVDF homopolymer has low/medium viscosity and is used in film extrusion and injection molding.Information provided by Solvay Specialty Polymers. |
|||
Glass Transition Temp, Tg | -40.0 °C | -40.0 °F | 10°C/min |
Arkema Group Kynar® 6000 HDC N 119 PVDF
(discontinued **) Designation ISO 12086-PVDF-E,GG1Z,Q.6E5.J.A.I.D, CD,Kynar PVDF are fluorinated thermoplastic homopolymers.Outstanding characteristics of Kynar: chemical resistance, imperviousness to UV, high barrie.. |
|||
Glass Transition Temp, Tg | -40.0 °C | -40.0 °F | Pellet sample |
BASF Elastollan® 1185A10Y Wire & Cable Grade Polyurethane Elastomer Compliant with NSF Standard 61 (Drinking water contact). As with all TPU products this grade must be dried prior to processing.Information provided by BASF Corporation. |
|||
Glass Transition Temp, Tg | -40.0 °C | -40.0 °F | DSC |
Lubrizol Estane® 58437 Thermoplastic Polyurethane Type: Estane® 58437 is an 85A aromatic polyester-based thermoplastic polyurethane (TPU).Features: Excellent cold temperature properties and improved heat resistance.Uses: Blown and flat die/cast fi.. |
|||
Glass Transition Temp, Tg | -40.0 °C | -40.0 °F | |
Sorbothane Polyurethane Damping Material, 70 Durometer Sorbothane® is a thermoset, polyether-based polyurethane viscoelastic material that combines high energy absorption with faultless memory. Sorbothane turns mechanical energy into heat. As the mat.. |
|||
Glass Transition Temp, Tg | -40.0 °C | -40.0 °F | 10°C/min |
Arkema Group Kynar® 4000 HD PVDF
(discontinued **) Designation ISO 12086-PVDF-E,GG1N,Q.?E5.I.B.E.C,, ?(6-10)Kynar PVDF are fluorinated thermoplastic homopolymers.Outstanding characteristics of Kynar: chemical resistance, imperviousness to UV, high b.. |