Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | -32.0 °C | -25.6 °F | DMTA |
Solvay Specialty Polymers Solef® 1015/0078 PVDF Homopolymer
(discontinued **) Key features of this grade: Plasticized, Offshore, Piping, Formulated. Recommended processing is extrusion. Available as granules.General information about SOLEF® PVDF: SOLEF® PVDF is a fluorina.. |
|||
Glass Transition Temp, Tg | -32.0 °C | -25.6 °F | Midpoint; ASTM E 1269 |
Huntsman IROGRAN® PS 455-215 TPU-Polyester Polyester-based grades with a broad processing window ideally suited for cast, flat die and flown film lines.Information provided by Alliance Polymers |
|||
Glass Transition Temp, Tg | -32.0 °C | -25.6 °F | |
Mallard Creek Polymers ROVENE® 4151 SBR Latex ROVENE® 4151 is a carboxylated styrene-butadiene emulsion that has a soft, resilient hand with above average strength properties. It may be compounded with a wide variety of fillers and additives.. |
|||
Glass Transition Temp, Tg | -32.0 °C | -25.6 °F | DSC heating rate = -10° C/min |
Kuraray HYBRAR® H7311 Hydrogenated Thermoplastic Rubber Description: HYBRAR® is another in the series of new high performance thermoplastic rubbers developed by KURARAY using their unique isoprene technology. HYBRAR® is a special thermoplastic rubb.. |
|||
Glass Transition Temp, Tg | -32.0 °C | -25.6 °F | ASTM D3418 |
DuPont Elvaloy® 741 Ethylene/Vinyl Acetate/Carbon Monoxide Copolymer Specialized copolymers deliver flexibility, toughness and weatherability to adhesives, plastics, highways and roofing.Availability: GloballyInformation provided by DuPont. |
|||
Glass Transition Temp, Tg | -32.0 °C | -25.6 °F | ASTM D3418 |
DuPont Elvaloy® 742 Ethylene/Vinyl Acetate/Carbon Monoxide Copolymer Specialized copolymers deliver flexibility, toughness and weatherability to adhesives, plastics, highways and roofing.Availability: GloballyInformation provided by DuPont. |
|||
Glass Transition Temp, Tg | -32.0 °C | -25.6 °F | By DSC |
DuPont Vamac® DP Sartomer 350 Coagent Test Compound Vamac® DP is an ethylene acrylic dipolymer elastomer. Its general performance characteristics are similar to those of the Vamac® terpolymers, including:Good oil and chemical resistanceHigh temper.. |
|||
Glass Transition Temp, Tg | -32.0 - -25.3 °C | -25.6 - -13.5 °F | Zeon Test #1273 |
Zeon Chemicals HyTemp® 4052 AR Polyacrylate Elastomer HyTemp 4052 contains acrylic esters with a small percentage of a chlorine/carboxy cure site monomer. Vulcanizates have excellent oil, heat, and compression set resistance with good low temperature.I.. |
|||
Glass Transition Temp, Tg | -32.0 °C | -25.6 °F | Ultimate Tg |
Tra-Con Tra-Bond 832-5 Flexible Epoxy TRA-BOND 832-5 is a flexible two component epoxy which is intended for bonding materials with mis-matched coefficients of expansion. It exhibits flexibility associated with polyurethanes but does no.. |
|||
Glass Transition Temp, Tg | -32.0 °C | -25.6 °F | DSC |
Lubrizol ESTANE® 58149 Ester Based Thermoplastic Polyurethane Features: Low Compression SetUse: Hydraulic Seals and Gaskets Available in Americas, Europe, Middle East, Africa, India and AsiaInformation provided by Lubrizol. |
|||
Glass Transition Temp, Tg | -32.0 °C | -25.6 °F | ASTM D3418 |
DuPont™ Elvaloy® 741WR Ethylene/Vinyl Acetate/Carbon Monoxide (E/VA/CO) Copolymer DuPont™ Elvaloy® 741WR an ethylene/vinyl acetate/carbon monoxide (E/VA/CO) copolymer. The difference between Elvaloy®741 and Elvaloy®741WR, is that Elvaloy®741WR contains a wax additive to dete.. |
|||
Glass Transition Temp, Tg | -32.0 °C | -25.6 °F | DSC |
Lubrizol ESTANE® 58206 Ester Based Thermoplastic Polyurethane Features: Good Flexibility at Low Temperatures and Improved Weathering Performance.Uses: Flat Die/Cast Film Extrusion and Hose/Profile Extrusion, Injection Molding.Available in Americas, Europe, Mid.. |