Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | -31.1 °C | -24.0 °F | DSC, 18ºF/min; DIN 51.007 |
Lubrizol Advanced Materials PEARLTHANE® 18VT80 Thermoplastic Polyurethane Elastomer
(discontinued **) PEARLTHANE® 18VT80 is a polyether based TPU, supplied in form of translucent, colorless pellets, combining hardness with excellent mechanical properties and superior hydrolysis and microbe resistan.. |
|||
Glass Transition Temp, Tg | -31.1 °C | -24.0 °F | DSC, 50°F/10min; ISO 11357-2 |
Lubrizol Advanced Materials PEARLTHANE® 16N95UV Thermoplastic Polyurethane Elastomer PEARLTHANE® 16N95UV is a polyether-based TPU, containing an anti-UV additive, supplied in form of translucent, colorless pellets, combining hardness with excellent mechanical properties and excel.. |
|||
Glass Transition Temp, Tg | -31.1 °C | -24.0 °F | DSC, 10ºC/min; DIN 51.007 |
Lubrizol Advanced Materials PEARLCOAT® Activa D118K Thermoplastic Polyurethane Elastomer PEARLCOAT® Activa D118K is a polycaprolactone copolyester based thermoplastic polyurethane of low hardness, supplied in form of natural pellets. This product gives an inherent “low gloss asp.. |