Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | -27.2 °C | -17.0 °F | DSC, 10ºC/min; DIN 51.007 |
Lubrizol Advanced Materials PEARLCOAT® 125K Thermoplastic Polyurethane Elastomer PEARLCOAT® 125K is a polyester based TPU, supplied in form of translucent, colorless pellets, featuring medium softening point, and consistent quality pellets, low gel content as well low-tempera.. |
|||
Glass Transition Temp, Tg | -27.2 °C | -17.0 °F | By DSC |
DuPont Vamac® GXF Sample Compound Vulcanizate Slab Cure (5 minutes at 190°C) Without Armeen® 18D Test slab is cured for 5 minutes at 190°C and post cured for 4hrs at 175°C. Vulcanizate performance test data can help end-users evaluate the potential fitness of similar compounds for their own .. |