Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | -25.0 °C | -13.0 °F | Second Run; DSC (-80°C to +100°C) |
RedEye On Demand PolyJet™ Resin, Black, Rapid Prototyping Material Tango PolyJet Resin (TangoGray™ FC950 & TangoBlack™ FC970) is a photopolymer resin designed for precise jetting in super fine layers by PolyJet™ Technology. Parts from the Tango PolyJet Resins si.. |
|||
Glass Transition Temp, Tg | -25.0 °C | -13.0 °F | Midpoint; ASTM E 1269 |
Huntsman IROGRAN® PS 443-201 TPU-Polyester Polyester-based grades with a broad processing window ideally suited for cast, flat die and flown film lines.Information provided by Alliance Polymers |
|||
Glass Transition Temp, Tg | -25.0 °C | -13.0 °F | |
Mallard Creek Polymers ROVENE® 4306 SBR Latex ROVENE® 4306 is a carboxylated styrene-butadiene emulsion that has a soft, resilient hand with outstanding strength properties. This self-crosslinking binder imparts excellent water and solvent r.. |
|||
Glass Transition Temp, Tg | -25.0 °C | -13.0 °F | |
Mallard Creek Polymers ROVENE® 5550 SBR Latex ROVENE® 5550 is a carboxylated styrene-butadiene emulsion that has a soft, resilient hand with outstanding strength properties. This Self-crosslinking binder imparts excellent water and solvent r.. |
|||
Glass Transition Temp, Tg | -25.0 °C | -13.0 °F | ASTM D1329 |
Seals Eastern 5353 Nitrile Rubber General purpose NitrileInformation provided by Seals Eastern, Inc. |
|||
Glass Transition Temp, Tg | -25.0 °C | -13.0 °F | ASTM D1329 |
Seals Eastern 7202 Nitrile Rubber Nitrile for oil & gas serviceInformation provided by Seals Eastern, Inc. |
|||
Glass Transition Temp, Tg | -25.0 °C | -13.0 °F | ASTM E1356 |
SK Chemicals SKYTHANE® U0417E Adhesive (Dry Lamination) Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. Applications include:Keyboard CoversOutsoles of Soccer ShoesWire and CableAirbagsSheets .. |
|||
Glass Transition Temp, Tg | -25.0 °C | -13.0 °F | ASTM D4065 |
SK Chemicals SKYTHANE® UB410 Powder Coating Description: SK Chemicals has supplied Thermoplastic Polyurethane Elastomer (TPU) under the name of SKYTHANE. UB series are used for adhesives and coating applications such as binder for magnetic ta.. |
|||
Glass Transition Temp, Tg | -25.0 °C | -13.0 °F | |
Styron XZ 92076.00 Carboxylated SB Performance Features: Soft, good cellulosic binderApplications: Wipes and TissueEuropeInformation provided by Styron |
|||
Glass Transition Temp, Tg | -25.0 °C | -13.0 °F | ASTM D1329 |
Seals Eastern 7157 Nitrile Rubber Nitrile for oil & gas serviceInformation provided by Seals Eastern, Inc. |
|||
Glass Transition Temp, Tg | -25.0 °C | -13.0 °F | HR 10 K/min, half height |
Styron Sprintan® SLR 4601 Solution Styrene Butadiene Rubber (S-SBR) Composition: SPRINTAN® SLR-4601 – Schkopau is manufactured by anionic solution polymerization using an organo-lithium initiator. The product has a medium styrene/high vinyl micro structure a.. |
|||
Glass Transition Temp, Tg | -25.0 °C | -13.0 °F | HR 10 K/min, half height |
Styron Sprintan® SLR 4602 Solution Styrene Butadiene Rubber (S-SBR) Composition: SPRINTAN® SLR-4602 – Schkopau is manufactured by anionic solution polymerization using an organo-lithium initiator. The product has a medium styrene/high vinyl micro structure a.. |
|||
Glass Transition Temp, Tg | -25.0 °C | -13.0 °F | ASTM D4065 |
SK Chemicals SKYTHANE® 410 Hotmelt Grade UB Polyurethane SKYTHANE is a thermoplastic polyurethane elastomer (TPU). Like materials ranging from rubber to plastics, it has excellent physical properties such as anti-abrasion, oil-resistance and mechanical pr.. |
|||
Glass Transition Temp, Tg | -25.0 °C | -13.0 °F | |
Wanhua Chemical Wanthane® WHT-8264 Polyether-Based TPU Excellent transparency, short cycle time, hydrolytic stability, fungus resistance, low temperature flexibility, UV resistanceInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
Glass Transition Temp, Tg | -25.0 °C | -13.0 °F | DSC |
Lubrizol ESTANE® 58226 Ester Based Thermoplastic Polyurethane Features: Excellent physical properties, good chemical resistance and enhanced hydrolysis resistance. Wide processing window for extrusion.Uses: Blown and flat die/cast film extrusion, Injection and.. |
|||
Glass Transition Temp, Tg | -25.0 °C | -13.0 °F | |
Lubrizol Estane® 2103-90A Thermoplastic Polyurethane Elastomer Formerly PellethaneFeature: Low compression setAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 20.. |
|||
Glass Transition Temp, Tg | -25.0 - -18.0 °C | -13.0 - -0.400 °F | |
Eliokem Sunigum® P7395 Acrylate Terpolymer Acrylate terpolymer partitioned with calcium carbonate. White powder; 1.00 mm particle size; medium viscosity.Intrinsically resistant to degradation by heat or UV radiation and to many chemicals in.. |
|||
Glass Transition Temp, Tg | -25.0 °C | -13.0 °F | HR 10 K/min; half height; DSC |
Dow SE SLR-4601 Solution polymerized Styrene Butadiene Rubber (S-SBR) SE SLR-4601 is manufactured by anionic solution polymerization using lithium initiator. It is a product with medium styrene and high vinyl content. The product is partially Sn-coupled and chemical.. |
|||
Glass Transition Temp, Tg | -25.0 °C | -13.0 °F | ASTM D1329 |
Seals Eastern 7168 Nitrile Rubber Nitrile for oil & gas serviceInformation provided by Seals Eastern, Inc. |