Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | -74.0 °C | -101 °F | Cured property; JMTP P200 |
Aptek 2503R-A/B Premeasured conformal urethane coating repair kit APTEK 2503-A/B is an unfilled, two component, electrically insulating, transparent, flexible urethane coating system designed for the encapsulation and protection of electrical/electronic components.. |
|||
Glass Transition Temp, Tg | -74.0 °C | -101 °F | Cured property; ASTM E831-86 |
Aptek 2503-A/B Low modulus urethane conformal coating APTEK 2503-A/B is an unfilled, two component, electrically insulating, transparent, flexible urethane coating system designed for the encapsulation and protection of electronic services mounted on p.. |