Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | 79.0 - 81.1 °C | 174 - 178 °F | Average value: 80.0 °C Grade Count:5 |
Overview of materials for PETG Copolyester This property data is a summary of similar materials in the MatWeb database for the category "PETG Copolyester". Each property range of values reported is minimum and maximum values of appropriate M.. |