Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | 55.0 - 60.0 °C | 131 - 140 °F | ASTM D3418 |
NatureWorks® Ingeo™ 2003D General Purpose Transparent Extrusion Grade Biopolymer NatureWorks® PLA polymer 2003D is a thermoplastic resin derived from annually renewable resources. PLA polymer 2003D processes easily on conventional extrusion equipment. Specifically designed fo.. |
|||
Glass Transition Temp, Tg | 55.0 - 60.0 °C | 131 - 140 °F | ASTM D3418 |
NatureWorks® Ingeo™ 3052D Lubricated, High Flow Biopolymer NatureWorks® PLA polymer 2003D is a thermoplastic resin derived from annually renewable resources. It is designed for injection molding applications where the requirements are clarity with heat def.. |
|||
Glass Transition Temp, Tg | 55.0 - 60.0 °C | 131 - 140 °F | ASTM D3417 |
NatureWorks® Ingeo™ 6060D Fiber Grade PLA NatureWorks PLA polymer 6060D is an amorphous thermoplastic fiber-grade resin derived primarily from annually renewable resources. Available in pellet form, 6060D is designed for extrusion into mech.. |
|||
Glass Transition Temp, Tg | 55.0 - 60.0 °C | 131 - 140 °F | ASTM D3417 |
NatureWorks® Ingeo™ 6201D Fiber Grade PLA NatureWorks® PLA polymer 6201D is a thermoplastic fiber-grade resin derived primarily from annually renewable resources. Available in pellet form, 6201D is designed for extrusion into mechanically .. |
|||
Glass Transition Temp, Tg | 55.0 - 60.0 °C | 131 - 140 °F | ASTM D3417 |
NatureWorks® Ingeo™ 6202D Fiber Grade PLA NatureWorks® PLA polymer 6202D is a thermoplastic fiber-grade resin derived primarily from annually renewable resources. Available in pellet form, 6202D is designed for extrusion into mechanically .. |
|||
Glass Transition Temp, Tg | 55.0 - 60.0 °C | 131 - 140 °F | ASTM D3417 |
NatureWorks® Ingeo™ 6204D Fiber Grade PLA NatureWorks® PLA polymer 6204D is a thermoplastic fiber-grade resin derived primarily from annually renewable resources. Available in pellet form, 6204D is designed for extrusion into mechanically .. |
|||
Glass Transition Temp, Tg | 55.0 - 60.0 °C | 131 - 140 °F | ASTM D3417 |
NatureWorks® Ingeo™ 6251D Fiber Grade PLA NatureWorks® PLA polymer 6251D is a thermoplastic fiber-grade resin derived primarily from annually renewable resources. Available in pellet form, 6251D is designed for spunbond products using conv.. |
|||
Glass Transition Temp, Tg | 55.0 - 60.0 °C | 131 - 140 °F | ASTM D3417 |
NatureWorks® Ingeo™ 6302D Fiber Grade PLA NatureWorks PLA polymer 6302D is an amorphous thermoplastic fiber-grade resin derived primarily from annually renewable resources. Available in pellet form, 6302D is designed for extrusion into mech.. |
|||
Glass Transition Temp, Tg | 55.0 - 60.0 °C | 131 - 140 °F | ASTM D3417 |
NatureWorks® Ingeo™ 6751D Fiber Grade PLA NatureWorks® PLA polymer 6751D is a thermoplastic fiber-grade resin derived primarily from annually renewable resources. Available in pellet form, 6751D is designed for extrusion into mechanically .. |
|||
Glass Transition Temp, Tg | 55.0 - 60.0 °C | 131 - 140 °F | ASTM D3417 |
NatureWorks® Ingeo™ 7032D Stretch Blow Molding/Bottle Grade PLA NatureWorks® PLA polymer 7032D is a bottles grade resin designed for injection stretch blow molded applications where heat setting is needed. PLA polymer 7032D can be run on conventional ISBM equip.. |
|||
Glass Transition Temp, Tg | 55.0 - 60.0 °C | 131 - 140 °F | ASTM D3418 |
NatureWorks® Ingeo™ 8052D Foam Grade Biopolymer Ingeo 8052D can be converted into an expanded foam sheet with use temperatures up to 77°F (25°C). This foam is lightweight, strong and suitable for packaging fresh meat and vegetables. In order to.. |
|||
Glass Transition Temp, Tg | 22.0 - 60.0 °C | 71.6 - 140 °F | Average value: 43.0 °C Grade Count:4 |
Overview of materials for Polybutylene Terephthalate (PBT), 40% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 40% Glass Fiber Filled". Specific grades with glass content between 35.. |
|||
Glass Transition Temp, Tg | 55.0 - 60.0 °C | 131 - 140 °F | ASTM D3417 |
NatureWorks® Ingeo™ 6252D Meltblown Fiber Grade Biopolymer NatureWorks® PLA polymer 6252D is a thermoplastic fiber-grade resin derived from annually renewable resources. Available in lubricated pellet form, 6252D is designed for meltblown products using co.. |
|||
Glass Transition Temp, Tg | 55.0 - 60.0 °C | 131 - 140 °F | ASTM D3417 |
NatureWorks® Ingeo™ 6350D Fiber Grade PLA NatureWorks PLA polymer 6350D is an amorphous thermoplastic spunbond-grade resin derived primarily from annually renewable resources. Available in pellet form, 6350D is designed for extrusion into s.. |
|||
Glass Transition Temp, Tg | 55.0 - 60.0 °C | 131 - 140 °F | ASTM D3417 |
NatureWorks® Ingeo™ 6400D Fiber Grade PLA NatureWorks® PLA polymer 6400D is a thermoplastic fiber-grade resin derived primarily from annually renewable resources. Available in pellet form, 6400D is designed for extrusion into mechanically .. |
|||
Glass Transition Temp, Tg | 55.0 - 60.0 °C | 131 - 140 °F | ASTM D3417 |
NatureWorks® Ingeo™ 6752D Spunbond Grade Biopolymer Sheath polymer for spunbound uses. NatureWorks® PLA polymer 6752D, a NatureWorks LLC product, is a thermoplastic fiber-grade resin de-rived from annually renewable resources. Available in pellet f.. |
|||
Glass Transition Temp, Tg | 55.0 - 60.0 °C | 131 - 140 °F | ASTM D3418 |
NatureWorks® Ingeo™ 7001D ISBM Bottle Grade Biopolymer Ingeo biopolymer 7001D is a thermoplastic resin derived from annually renewable resources and is specifically designed for use in injection stretch blow molded (ISBM) bottle applications. Ingeo biop.. |
|||
Glass Transition Temp, Tg | 57.0 - 60.0 °C | 135 - 140 °F | ASTM E1545-00 |
DSM Somos® 9420 Epoxy Resin for Stereolithography DescriptionDSM Somos® 9420 is a liquid photopolymer that produces robust, functional and accurate parts using stereolithography machines. The material offers superior chemical resistance and a wid.. |
|||
Glass Transition Temp, Tg | 54.0 - 60.0 °C | 129 - 140 °F | Average value: 56.0 °C Grade Count:6 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass + Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass + Mineral Filled". Each property range of values reported is min.. |