Thermal Properties Metric English Comments
Glass Transition Temp, Tg 76.1 - 170 °C
169 - 338 °F
Average value: 107 °C Grade Count:7
Overview of materials for Epoxy/Carbon Fiber Composite
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy/Carbon Fiber Composite". Each property range of values reported is minimum and maximum values of a..
Glass Transition Temp, Tg 60.0 - 170 °C
140 - 338 °F
Average value: 97.6 °C Grade Count:12
Overview of materials for Epoxy, Molded, Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Molded, Glass Fiber Filler". Each property range of values reported is minimum and maximum values..