Thermal Properties Metric English Comments
Glass Transition Temp, Tg 93.0 - 153 °C
199 - 307 °F
Average value: 131 °C Grade Count:6
Overview of materials for Nylon 6-3
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6-3". Each property range of values reported is minimum and maximum values of appropriate MatWeb e..