Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | 143 - 150 °C | 289 - 302 °F | Average value: 145 °C Grade Count:5 |
Overview of materials for Polyetheretherketone, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, PTFE Filled". Each property range of values reported is minimum and maximum values.. |
|||
Glass Transition Temp, Tg | 145 - 150 °C | 293 - 302 °F | Average value: 148 °C Grade Count:4 |
Overview of materials for Polycarbonate, Carbon Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, Carbon Fiber Reinforced". Each property range of values reported is minimum and maximum v.. |
|||
Glass Transition Temp, Tg | 145 - 150 °C | 293 - 302 °F | Average value: 148 °C Grade Count:5 |
Overview of materials for Polycarbonate/Styrenic Alloy This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Styrenic Alloy". Each property range of values reported is minimum and maximum values of a.. |
|||
Glass Transition Temp, Tg | 108 - 150 °C | 226 - 302 °F | Average value: 136 °C Grade Count:5 |
Overview of materials for Nylon, Amorphous Transparent Alloy This property data is a summary of similar materials in the MatWeb database for the category "Nylon, Amorphous Transparent Alloy". Each property range of values reported is minimum and maximum value.. |
|||
Glass Transition Temp, Tg | 145 - 150 °C | 293 - 302 °F | |
A. Schulman ComAlloy Comtuf® 410 Polycarbonate/Polyester Alloy Data provided by the manufacturer, ComAlloy International Company. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been integrated into the A Sc.. |
|||
Glass Transition Temp, Tg | 145 - 150 °C | 293 - 302 °F | |
A. Schulman ComAlloy Comtuf® 520 Polycarbonate/Styrenic Alloy Data provided by the manufacturer, ComAlloy International Company. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been integrated into the A Sc.. |
|||
Glass Transition Temp, Tg | 145 - 150 °C | 293 - 302 °F | |
A. Schulman ComAlloy Comtuf® 522 Polycarbonate/Styrenic Alloy Data provided by the manufacturer, ComAlloy International Company. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been integrated into the A Sc.. |
|||
Glass Transition Temp, Tg | 145 - 150 °C | 293 - 302 °F | |
A. Schulman ComAlloy Comtuf® 523 Polycarbonate/Styrenic Alloy Data provided by the manufacturer, ComAlloy International Company. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been integrated into the A Sc.. |
|||
Glass Transition Temp, Tg | 145 - 150 °C | 293 - 302 °F | |
A. Schulman ComAlloy Comtuf® 525 Polycarbonate/Styrenic Alloy Data provided by the manufacturer, ComAlloy International Company. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been integrated into the A Sc.. |
|||
Glass Transition Temp, Tg | 145 - 150 °C | 293 - 302 °F | |
A. Schulman ComAlloy E-16831B Polycarbonate, Electrically Conductive - Carbon Fiber Filled Data provided by the manufacturer, ComAlloy International Company.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Glass Transition Temp, Tg | 145 - 150 °C | 293 - 302 °F | |
A. Schulman ComAlloy Hiloy® 511 Polycarbonate, Glass Reinforced, UL Data provided by the manufacturer, ComAlloy International Company.10% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Glass Transition Temp, Tg | 145 - 150 °C | 293 - 302 °F | |
A. Schulman ComAlloy Hiloy® 512 Polycarbonate, Glass Reinforced, UL Data provided by the manufacturer, ComAlloy International Company.20% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Glass Transition Temp, Tg | 145 - 150 °C | 293 - 302 °F | |
A. Schulman ComAlloy Hiloy® 513 Polycarbonate, Glass Reinforced, UL Data provided by the manufacturer, ComAlloy International Company.30% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Glass Transition Temp, Tg | 145 - 150 °C | 293 - 302 °F | |
A. Schulman ComAlloy Hiloy® 514 Polycarbonate, Glass Reinforced, UL Data provided by the manufacturer, ComAlloy International Company.40% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Glass Transition Temp, Tg | 145 - 150 °C | 293 - 302 °F | |
A. Schulman ComAlloy Hiloy® 515 Polycarbonate, Carbon Fiber Reinforced Data provided by the manufacturer, ComAlloy International Company.10% Carbon Fiber Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Glass Transition Temp, Tg | 145 - 150 °C | 293 - 302 °F | |
A. Schulman ComAlloy Hiloy® 516 Polycarbonate, Carbon Fiber Reinforced Data provided by the manufacturer, ComAlloy International Company.20% Carbon Fiber Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Glass Transition Temp, Tg | 145 - 150 °C | 293 - 302 °F | |
A. Schulman ComAlloy Hiloy® 517 Polycarbonate, Carbon Fiber Reinforced Data provided by the manufacturer, ComAlloy International Company.30% Carbon Fiber Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Glass Transition Temp, Tg | 145 - 150 °C | 293 - 302 °F | |
A. Schulman ComAlloy Lubrilon® 511 Polycarbonate, Glass Fiber/PTFE, UL Data provided by the manufacturer, ComAlloy International Company. High performance and excellent lubricity with minimal surface wear.The ComAlloy product line has been integrated into the A Schulma.. |
|||
Glass Transition Temp, Tg | 145 - 150 °C | 293 - 302 °F | |
A. Schulman ComAlloy Lubrilon® 512 Polycarbonate, Glass Fiber/PTFE, UL Data provided by the manufacturer, ComAlloy International Company. High performance and excellent lubricity with minimal surface wear.The ComAlloy product line has been integrated into the A Schulma.. |
|||
Glass Transition Temp, Tg | 145 - 150 °C | 293 - 302 °F | |
A. Schulman ComAlloy Comtuf® 413 Glass Reinforced, Polycarbonate/Polyester Alloy, UL Data provided by the manufacturer, ComAlloy International Company.20% Glass Reinforced. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been int.. |
|||
Glass Transition Temp, Tg | 145 - 150 °C | 293 - 302 °F | |
A. Schulman ComAlloy Comtuf® 524 Polycarbonate/Styrenic Alloy Data provided by the manufacturer, ComAlloy International Company. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been integrated into the A Sc.. |
|||
Glass Transition Temp, Tg | 145 - 150 °C | 293 - 302 °F | |
A. Schulman ComAlloy Hiloy® 518 Polycarbonate, Carbon Fiber Reinforced Data provided by the manufacturer, ComAlloy International Company.40% Carbon Fiber Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |