Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | -42.0 - -39.0 °C | -43.6 - -38.2 °F | (DMA) @ 1 Hz |
Arkema Group Kynar Flex® 2900 PVDF Copolymer
(discontinued **) Copolymer Series, Kynar® components are used extensively in the high purity semiconductor market, the pulp and paper industry, nuclear waste processing, and the general chemical processing industry.. |
|||
Glass Transition Temp, Tg | -42.0 - -39.0 °C | -43.6 - -38.2 °F | (DMA) @ 1 Hz |
Arkema Group Kynar Flex® 3120 PVDF Copolymer
(discontinued **) Copolymer Series, Kynar® components are used extensively in the high purity semiconductor market, the pulp and paper industry, nuclear waste processing, and the general chemical processing industry.. |
|||
Glass Transition Temp, Tg | -41.0 - -39.0 °C @Frequency 1.00 Hz |
-41.8 - -38.2 °F @Frequency 1.00 Hz |
DMA |
Arkema Group KYNAR FLEX® 2800-00 Polyvinylidene Fluoride Copolymer - Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. Flexible. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low.. |
|||
Glass Transition Temp, Tg | -41.0 - -39.0 °C @Frequency 1.00 Hz |
-41.8 - -38.2 °F @Frequency 1.00 Hz |
DMA |
Arkema Group KYNAR FLEX® 2800-01 Polyvinylidene Fluoride Copolymer - Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. Flexible, lubricated. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical s.. |
|||
Glass Transition Temp, Tg | -41.0 - -39.0 °C @Frequency 1.00 Hz |
-41.8 - -38.2 °F @Frequency 1.00 Hz |
DMA |
Arkema Group KYNAR FLEX® 2900-04 Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. Flexible, flame and smoke suppressant. High stability in harsh thermal, chemical and ultraviolet environments. High toughness.. |
|||
Glass Transition Temp, Tg | -41.0 - -39.0 °C @Frequency 1.00 Hz |
-41.8 - -38.2 °F @Frequency 1.00 Hz |
DMA |
Arkema Group KYNAR FLEX® 3120-15 Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. Flexible, flame and smoke suppressant. High stability in harsh thermal, chemical and ultraviolet environments. High toughness.. |
|||
Glass Transition Temp, Tg | -41.0 - -39.0 °C @Frequency 1.00 Hz |
-41.8 - -38.2 °F @Frequency 1.00 Hz |
DMA |
Arkema Group KYNAR FLEX® 3120-50 Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. Flexible, 150°C temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness a.. |
|||
Glass Transition Temp, Tg | -41.0 - -39.0 °C @Frequency 1.00 Hz |
-41.8 - -38.2 °F @Frequency 1.00 Hz |
DMA |
Arkema Group KYNAR FLEX® 2800-20 Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. Flexible. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low.. |