Glass Transition Temp, Tg 83.0 - 145 °C
181 - 293 °F
Average value: 105 °C Grade Count:3
Overview of materials for Thermoset Polyurethane, Liquid
This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane, Liquid". Each property range of values reported is minimum and maximum values of..
Glass Transition Temp, Tg 83.0 - 100 °C
181 - 212 °F
Average value: 90.5 °C Grade Count:6
Overview of materials for Polystyrene, Molded, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene". Each property range of values reported is minimum and maximum values of appropriate MatWeb..
Glass Transition Temp, Tg 83.0 °C
181 °F
Plain Cast Resin; ASTM D3418
TSE Industries EcoWIND® M110 General Purpose Filament Winding Polyurethane Resin
TSE-EcoWIND® resins are “Environmentally-Preferred Products” or EPP’s. They are a pair of polyurethane resins free of Styrene, and are “ultra-low” emitting during application. TSE-EcoWIND® re..
Glass Transition Temp, Tg 83.0 °C
181 °F
Plain Cast Resin; ASTM D3418
TSE Industries EcoWIND® M110 General Purpose Filament Winding Polyurethane Resin
TSE-EcoWIND® resins are “Environmentally-Preferred Products” or EPP’s. They are a pair of polyurethane resins free of Styrene, and are “ultra-low” emitting during application. TSE-EcoWIND® re..
Glass Transition Temp, Tg 83.0 °C
181 °F
Eastman Eastar DN001 PCTG Copolyester
ISO data as provided by the manufacturer, Eastman Chemical
Glass Transition Temp, Tg 83.0 °C
181 °F
Eastman Eastar DN004 PCTG Copolyester
ISO data as provided by the manufacturer, Eastman Chemical
Glass Transition Temp, Tg 83.0 °C
181 °F
Armstrong A-12 Epoxy Adhesive, at 3:2 Mix Ratio
Our most popular general-purpose, high viscosity adhesive for industry. Combines low toxicity with excellent physical properties, and offers a non-critical mixing ratio of 1:1 by weight. This rati..
Glass Transition Temp, Tg 83.0 °C
181 °F
Ultimate Tg, 20°C/min; TMA
Tra-Con Tra-Bond 970-1N1 General Purpose Epoxy Adhesive
TRA-BOND 970-1N1 is a general purpose epoxy that exhibits sag resistance and excellent bond strength to a wide variety of substrates. Information provided by Tra-Con Inc.