Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | 77.0 - 81.0 °C | 171 - 178 °F | QCD--W1-21 |
Pearl Engineering PEPLPET D-101-SH Monofilament Resin Used in the paper industry as paper pulp nets. |
|||
Glass Transition Temp, Tg | 77.0 - 81.0 °C | 171 - 178 °F | QCD--W1-21 |
Pearl Engineering PEPLPET FR-101-H Monofilament Resin Used as textile grade flame retardant for furniture, car and plane upholstery. |
|||
Glass Transition Temp, Tg | 77.0 °C | 171 °F | |
Eastman Eastapak 7352 PET
(discontinued **) Unreinforced Low IV. ISO data as provided by the manufacturer, Eastman Chemical.This product is discontinued; 2003. |
|||
Glass Transition Temp, Tg | 77.0 - 81.0 °C | 171 - 178 °F | QCD--W1-21 |
Pearl Engineering PEPLPET B101H Monofilament Resin Generally used in monofilament v-belts, zips and other technical applications. |
|||
Glass Transition Temp, Tg | 77.0 °C | 171 °F | Ultimate Tg |
Tra-Con Tra-Bond 2113 Clear Low Viscosity Epoxy Adhesive TRA-BOND 2113 is a clear, low viscosity epoxy adhesive system that contains no solvents, cures at room temperature, has excellent flowability and wetting characteristics, and adheres strongly to gla.. |
|||
Glass Transition Temp, Tg | 77.0 °C | 171 °F | Ultimate Tg |
Tra-Con Tra-Bond 2114 Water White Transparent Epoxy Adhesive TRA-BOND 2114 is a transparent, low viscosity epoxy resin formulation recommended for industrial adhesive and laminating applications where sparkling clarity and excellent structural, mechanical and.. |
|||
Glass Transition Temp, Tg | 77.0 °C | 171 °F | Dry |
Hexcel® HexPly® F185 Epoxy Resin HexPly® F185 is an advanced epoxy formulation designed for autoclave curing to offer very high sandwich and metal bonding strengths with moderate laminate strengths. HexPly® F185 is a structural a.. |
|||
Glass Transition Temp, Tg | 77.0 °C | 171 °F | |
Eastman Eastar EN058 PET Copolymer ISO data as provided by the manufacturer, Eastman Chemical |
|||
Glass Transition Temp, Tg | 77.0 °C | 171 °F | Internal Method |
Eastman Embrace HY1000 Copolyester for Shrink Film Applications:Beverage packagingCosmetics/personal care packagingDairy packagingFood packagingJuice packagingPharmaceutical packagingKey Attributes:Eye catching 360° graphic capabilityNoise-free shr.. |
|||
Glass Transition Temp, Tg | 77.0 °C | 171 °F | |
Armstrong A-1/V Epoxy Adhesive A brown epoxy paste formulated with enhanced wetting capabilities to hard rubbers and rigid thermoplastics. Has low outgassing characteristics at temperatures below 250°FInformation provided by El.. |
|||
Glass Transition Temp, Tg | 77.0 °C | 171 °F | TM R050-25 |
Resinlab® EP11HT Gray Filled Epoxy Adhesive Resinlab™ EP11HT Gray is a two part filled epoxy adhesive designed for bonding metals and plastics. It cures at room temperature to a tough, semi-rigid material. It has good wetting to most surfa.. |