Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | 70.0 °C | 158 °F | ISO 11359-2:1999 |
Global EPP PET PET is an unreinforced, semi-crystalline thermoplastic polyester, demonstrating dimensional stability similar to acetal, combined with the comparable wear resistance of nylon. Heavily loaded mechani.. |
|||
Glass Transition Temp, Tg | 70.0 °C | 158 °F | ISO 11359-2:1999 |
Global EPP PET SL PET + Solid Lubricant PET is an unreinforced, semi-crystalline thermoplastic polyester, demonstrating dimensional stability similar to acetal, combined with the comparable wear resistance of nylon. Heavily loaded mechani.. |
|||
Glass Transition Temp, Tg | 70.0 °C | 158 °F | |
Lord Adhesives CircuitSAFâ„¢ MA-420 Epoxy Surface Mount Adhesive CircuitSAFâ„¢ MA-420 is an epoxy surface mount adhesive that cures rapidly at elevated temperatures and has been designed for use in high speed printed circuit board assembly for the attachment o.. |
|||
Glass Transition Temp, Tg | 70.0 °C | 158 °F | |
Lucite International Elvacite ® 2669 Acrylic Resin Elvacite® 2669, the first in this series, is a solid acrylic bead copolymer which can be dissolved in slightly alkaline aqueous systems. This distinct capability makes the product particularly su.. |
|||
Glass Transition Temp, Tg | 70.0 - 75.0 °C | 158 - 167 °F | |
Master Bond LED401 One Component LED Curable Adhesive System Master Bond LED401 is a highly innovative, one part LED type system that cures fully upon exposure to a 405 nm wavelength light source where the presence of any UV light is minimal or incidental. In.. |
|||
Glass Transition Temp, Tg | 70.0 - 75.0 °C | 158 - 167 °F | |
Master Bond LED401 White One Part, LED Curable Compound Description: Master Bond LED401 White is a one part LED type system that cures fully upon exposure to a 405 nm wavelength light source where the presence of any UV light is minimal or incidental. In.. |
|||
Glass Transition Temp, Tg | 70.0 - 75.0 °C | 158 - 167 °F | |
Master Bond LED403Med USP Class VI, One Component, LED Curable System Master Bond LED403Med is a one part LED system that cures fully upon exposure to a 405 nm wavelength light that is generated by an LED source and. In fact, this material will fully cure tack-free wi.. |
|||
Glass Transition Temp, Tg | 70.0 - 75.0 °C | 158 - 167 °F | |
Master Bond Supreme 11ANHT Fast Curing Epoxy Paste System Description: Master Bond Polymer System SUPREME 11ANHT is a two component epoxy resin system for high performance bonding and sealing formulated to cure at room temperature or more rapidly at elevat.. |
|||
Glass Transition Temp, Tg | 70.0 °C | 158 °F | |
Unitika elitel UE9600 Polyester, Pellet Low viscosity type UE3600 CoatabilityUNITIKA l resins are thermoplastic saturated copolymeric polyester resins. l resins are expanding their applications from products such as adhesives, paints, in.. |
|||
Glass Transition Temp, Tg | 70.0 °C | 158 °F | JIS K7121 |
Zeon Chemicals Zeonor® 750R Cyclo Olefin Polymer Zeonor® is a line of thermoplastic polyolefin resin with an excellent combination of optical and electronic properties. These unique Cyclo Olefin Polymer (COP) was developed by Zeon Corporation usi.. |
|||
Glass Transition Temp, Tg | 70.0 °C | 158 °F | Ultimate Tg |
Tra-Con Tra-Bond 216D01 Dam/Fill Applications Adhesive TRA-BOND 216D01 is for dam and fill applications. TRA-BOND 216D01 bonds exceptionally well to ceramic, glass, metal and plastic. Fully cured TRA-BOND 216D01 is an electrical insulator with superior .. |
|||
Glass Transition Temp, Tg | 70.0 °C | 158 °F | Ultimate Tg |
Tra-Con Tra-Bond 216D02 Thixotropic No-Sag Epoxy Adhesive TRA-BOND 216D02 is a thixotropic, two part epoxy adhesive formulated specifically for applications where a nonsagging adhesive is required. TRA-BOND 216D02 works in concert with TRA-CAST 3135 to per.. |
|||
Glass Transition Temp, Tg | 70.0 °C | 158 °F | Ultimate Tg |
Tra-Con Tra-Bond 342-14T Low Viscosity Room Temperature Cure Epoxy Adhesive TRA-BOND 342-14T single component, low viscosity alumina-filled epoxy adhesive exhibits high bond strength and excellent thermal shock characteristics. This adhesive may be cured at room temperature.. |
|||
Glass Transition Temp, Tg | 70.0 °C | 158 °F | Ultimate Tg |
Tra-Con Tra-Bond FDA2T Food and Drug Application Epoxy Adhesive TRA-BOND FDA-2T is a thixotropic epoxy resin system specifically developed for medical device applications. It has been tested in accordance with USP biological reactivity tests, in vivo and receive.. |
|||
Glass Transition Temp, Tg | 70.0 °C | 158 °F | Ultimate Tg |
Tra-Con Tra-Bond FS227 Thixotropic Epoxy/Polyamide Adhesive TRA-BOND FS227 is a thixotropic (thick paste) polymer epoxy/polyamide system developed for industrial adhesive and sealing applications where the combination of high fill, easy handling, good wettin.. |
|||
Glass Transition Temp, Tg | 70.0 °C | 158 °F | Ultimate Tg |
Tra-Con Tra-Duct 916H04 Room Temperature Cure, Conductive Silver Epoxy Adhesive TRA-DUCT 916H04 is an electrically conducting silver-filled epoxy compound recommended for electronic bonding and sealing applications that require a combination of good mechanical and electrical pr.. |
|||
Glass Transition Temp, Tg | 70.0 °C | 158 °F | |
Loctite® Durabond® E-30CL Epoxy Adhesive Epoxy AdhesivesLoctite offers a complete line of one-part and two-part epoxy and urethane adhesives for structural bonding, potting and encapsulating. The Loctite® Durabond® line contains 14 appli.. |
|||
Glass Transition Temp, Tg | 70.0 °C | 158 °F | ETM E-90 |
ExxonMobil ESCOREZ™ 1401 (Europe) Petroleum Hydrocarbon Resin ESCOREZ™ 1401 is a modified aliphatic hydrocarbon resin with a narrow molecular weight distribution and a high softening point. It is a tackifying resin designed to provide high temperature perform.. |
|||
Glass Transition Temp, Tg | 70.0 °C | 158 °F | DSC 3146 |
Bond Laminates TEPEX® dynalite 201-C200(x)/45% Carbon – PA6.6 Consolidated Composite Laminate Within the TEPEX® composite laminate, Polyamide 66 is a resin known for its high hardness, stiffness, abrasion resistance, heat and chemical resistances. The carbon used within this material is ae.. |
|||
Glass Transition Temp, Tg | 70.0 °C | 158 °F | |
Atom Adhesives AA-BOND FDA2T Epoxy Adhesive AA-BOND FDA2T is a thixotropic epoxy resin system specifically developed for medical device applications. It has been tested in accordance with USP biological reactivity tests, in vivo and received .. |
|||
Glass Transition Temp, Tg | 70.0 °C | 158 °F | 10°C/min; DAM; ISO 11357-1/-2 |
DuPont Performance Polymers Zytel® FG77G33L NC010 Nylon 612
(Unverified Data**) Zytel® FG77G33L NC010 is a 33% glass fiber reinforced polyamide 612 resin for injection molding. It has been developed for consideration for applications such as parts in the food industry.Informat.. |
|||
Glass Transition Temp, Tg | 70.0 °C | 158 °F | TM R050-25 |
Resinlab® EP1195 Flame Retardant Epoxy Casting Resin Resinlab™ EP1195 is a low viscosity, fast gelling, flame retardant epoxy casting resin system. It is recognized under the Component Recognition Program of Underwriters Laboratories Inc., (File # E1.. |
|||
Glass Transition Temp, Tg | 70.0 °C | 158 °F | Tg tan d, Dry, Cured Neat Resin Property, 5 days @ 22°C/72°F |
Hexcel® Redux® 810 Two-Part Epoxy Paste Adhesive Redux® 810 is a multi-purpose, high shear and peel strength, two-part, toughened epoxy paste adhesive with corrosion-inhibiting properties.Features: Available in cartridges with a static mixer and .. |
|||
Glass Transition Temp, Tg | 70.0 °C | 158 °F | |
Loctite® Durabond® E-60HP Epoxy Adhesive Epoxy AdhesivesLoctite offers a complete line of one-part and two-part epoxy and urethane adhesives for structural bonding, potting and encapsulating. The Loctite® Durabond® line contains 14 appli.. |