Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | 7.00 °C | 44.6 °F | Film; DSC |
Solvay Specialty Polymers Diofan® A602 Polyvinylidene Chloride (PVDC)
(discontinued **) DIOFAN® A602 is a water based dispersion of a polyvinylidene chloride copolymer. It is free of solvent traces, alkylphenol ethoxylates or any other toxic substances. It features strong barrier prop.. |
|||
Glass Transition Temp, Tg | 7.00 °C | 44.6 °F | |
Mallard Creek Polymers ROVENE® 6087 Styrene-Acrylic Emulsion ROVENE® 6087 is a high solids, low VOC styrene-acrylic copolymer emulsion that provides outstanding wet strength and moisture barrier properties.APPLICATIONS: ROVENE® 6087 typical applications.. |
|||
Glass Transition Temp, Tg | 7.00 °C | 44.6 °F | |
Mallard Creek Polymers ROVENE® 6487 Styrene-Acrylic Emulsion ROVENE® 6487 is a high solids, low VOC styrene-acrylic copolymer emulsion that provides outstanding wet strength and moisture barrier properties.APPLICATIONS: ROVENE® 6487 typical applications.. |
|||
Glass Transition Temp, Tg | 7.00 °C | 44.6 °F | DSC heating rate = -10° C/min |
Kuraray SEPTON® H5127 Description: HYBRAR® is another in the series of new high performance thermoplastic rubbers developed by KURARAY using their unique isoprene technology. HYBRAR® is a special thermoplastic rubb.. |
|||
Glass Transition Temp, Tg | 7.00 °C | 44.6 °F | DSC |
Solvay Specialty Polymers Diofan® A 602 Polyvinylidene Chloride (PVDC) Diofan® A 602 is a water based dispersion of a polyvinylidene chloride copolymer. It is free of solvent traces, alkylphenol ethoxylates or any other toxic substances.It features strong barrier pr.. |
|||
Glass Transition Temp, Tg | 7.00 °C | 44.6 °F | |
Styron DL 238NA Carboxylated SB Performance Features: Strong bonding with clays and fillersApplications: General Purpose AdhesiveNorth AmericaInformation provided by Styron |
|||
Glass Transition Temp, Tg | 7.00 °C | 44.6 °F | |
Styron Modifier A/NA SB Latex Performance Features: Excellent alkaline stability, excellent adhesion and strength, freeze/thaw stability, controlled air entrainment, meets FHWA RD-78-35Applications: Modified ConcreteNorth Americ.. |
|||
Glass Transition Temp, Tg | 7.00 °C | 44.6 °F | |
Styron DL 2703LA Carboxylated SB Performance Features: Excellent bonding, high film elongation, heat sealable, low odor, high water resistanceApplications: General Purpose AdhesiveLatin America/South AmericaInformation provided by .. |
|||
Glass Transition Temp, Tg | 7.00 °C | 44.6 °F | Onset |
3M Scotch-Weld™ DP190 Gray Epoxy Adhesive 3M™ Scotch-Weld™ Epoxy Adhesive DP190 Gray is a 1:1 mix ratio similar to Scotch-Weld™ Epoxy Adhesive 2216 B/A Gray and exhibits good peel, shear and environmental aging properties.Information pro.. |
|||
Glass Transition Temp, Tg | 7.00 - 16.0 °C | 44.6 - 60.8 °F | Average value: 12.8 °C Grade Count:8 |
Overview of materials for Polyvinyl Dichloride (PVDC) This property data is a summary of similar materials in the MatWeb database for the category "Polyvinyl Dichloride (PVDC)". Each property range of values reported is minimum and maximum values of ap.. |
|||
Glass Transition Temp, Tg | 7.00 °C | 44.6 °F | |
Styron Latex DL 2703LA Carboxylated SB Performance Features: Excellent binding strength and durabilityApplications: Dust Control and Soil StabilizationLatin America/South AmericaInformation provided by Styron |
|||
Glass Transition Temp, Tg | 7.00 °C | 44.6 °F | |
Styron Modifier A SB Latex Performance Features: Excellent alkaline stability, excellent adhesion and strength, freeze/thaw stability, controlled air entrainment, meets FHWA RD-78-35Applications: Latex Modified Concrete (LMC).. |
|||
Glass Transition Temp, Tg | 7.00 °C | 44.6 °F | |
Mallard Creek Polymers ROVENE® 4457 SBR Latex ROVENE® 4457 is a highly carboxylated styrene-butadiene emulsion that has a firm hand with excellent strength properties. This binder is a low VOC containing latex that is crosslinkable with extern.. |