Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | 66.0 - 87.0 °C | 151 - 189 °F | DMA, E" |
Proto3000 Accura® 45HC Plastic Stereolithography (SLA) Prototyping Polymer A high speed material, with excellent thermal and moisture resistance for producing functional prototypes in 3D Systems' SLA 250 systems.Benefits:Fast build speed:Provides build speeds that are sign.. |
|||
Glass Transition Temp, Tg | 66.0 °C | 151 °F | TM R050-25 |
Resinlab® EP1390 Medium Viscosity, Self Extinguishing Flame Retardant Epoxy Casting Resin System Resinlab™ EP1390 is a RoHS compliant, medium viscosity, self extinguishing flame retardant epoxy casting resin system. It is recognized under the Component Recognition Program of Underwriters Labor.. |
|||
Glass Transition Temp, Tg | 66.0 °C | 151 °F | |
Lucite International Elvacite ® 2043 Acrylic Resin Elvacite® 2043 is a low molecular weight ethyl methacrylate copolymer. It is a fast – dissolving, low viscosity resin with alcohol solubility for flexographic inks. Most compatible grade. It.. |
|||
Glass Transition Temp, Tg | 66.0 °C | 151 °F | Ultimate Tg |
Tra-Con Tra-Bond 224-1 Rapid Room Temperature Cure Epoxy Adhesive TRA-BOND 224-1 room temperature curing epoxy adhesive develops structural strength rapidly. Unlike most "rapid cure" epoxies which gel in one or two minutes, TRA-BOND 224-1 adhesive exhibits a 30 mi.. |
|||
Glass Transition Temp, Tg | 66.0 °C | 151 °F | Ultimate Tg |
Tra-Con Tra-Bond 868-3N1 Room Temperature Cure Adhesive TRA-BOND 868-3N1 room temperature cure adhesive provides strong bonds to difficult-to-bond metals, such as gold, silver, copper, brass, and solder.Information provided by Tra-Con Inc. |
|||
Glass Transition Temp, Tg | 66.0 °C | 151 °F | ETM 300-90 |
ExxonMobil ESCOREZ™ 5415 Petroleum Hydrocarbon Resin Light colored cycloaliphatic hydrocarbon resin. They are designed to tackify a variety of adhesive polymers including EVA, SIS and SEBS block copolymers, natural rubber, synthetic polyisoprene, poly.. |
|||
Glass Transition Temp, Tg | 66.0 - 87.0 °C | 151 - 189 °F | DMA, E" |
3D Systems Accura® 45HC Plastic for SLA® Systems A high speed material, with excellent thermal and moisture resistance for producing functional prototypes in 3D Systems' SLA 250 systems.ApplicationsHigh temperature testing:Automotive "under-the-ho.. |
|||
Glass Transition Temp, Tg | 66.0 °C | 151 °F | Ultimate Tg |
Tra-Con Tra-Bond 224-8 Room Temperature Cure Epoxy Adhesive TRA-BOND 224-8 room temperature cure epoxy adhesive is a thermally conductive version of 224-1. This adhesive develops structural strength rapidly. When cured at room temperature, this adhesive prov.. |