Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | 6.00 °C | 42.8 °F | |
Styron DL 374 Carboxylated SB Performance Features: Heat sealable, low odor, high water resistance, casein compatibility, isocyanate adhesive modifierApplications: Foil Lamination (FSK), Heat Sealable, Lamination (Metalized Pape.. |
|||
Glass Transition Temp, Tg | 6.00 °C | 42.8 °F | |
Styron XZ 91988.02 Cross-Linking SB Performance Features: Excellent alkali resistance, low blockingApplications: Fiber Binding, Glass Fiber Binding and Performance CoatingsEuropeInformation provided by Styron |
|||
Glass Transition Temp, Tg | 6.00 °C | 42.8 °F | |
Styron XZ 92059.00 Carboxylated SB Performance Features: Heat sealable, low odor, high water resistance, casein compatibilityApplications: Foil Lamination (FSK), Heat Sealable and Lamination (Metalized Paper)EuropeInformation provide.. |
|||
Glass Transition Temp, Tg | 6.00 °C | 42.8 °F | |
Styron XZ 91982.00 Carboxylated SB Performance Features: PH controlled re-pulpability, solvent resistance, casein compatibilityApplications: Foil Lamination (FSK) and Lamination (Metalized Paper) EuropeInformation provided by Styron |
|||
Glass Transition Temp, Tg | 6.00 °C | 42.8 °F | |
Styron XZ 94445.00 Carboxylated SB Performance Features: Control of moisture vapor permeability, high water resistanceApplications: Waterproofing MembranesEuropeInformation provided by Styron |
|||
Glass Transition Temp, Tg | 6.00 °C | 42.8 °F | |
Styron XZ 97214.00 Carboxylated SB Performance Features: Good cement stability and adhesion, high binding power, formulation versatilityApplications: PrimerEuropeInformation provided by Styron |
|||
Glass Transition Temp, Tg | 6.00 °C | 42.8 °F | Ultimate Tg |
Tra-Con Tra-Bond 2159 Heat Conductive Electrically Insulating Compound TRA-BOND 2159 is a flexible, thermal conductive epoxy system. It is used for staking transistors, diodes, resistors, integrated circuits and other heat-sensitive components to printed circuit boards.. |
|||
Glass Transition Temp, Tg | 6.00 °C | 42.8 °F | |
Dow FOUNDATIONS 885 High Performance Latex for Carpet Carboxylated Styrene/Acrylate Latex Applications: FOUNDATIONS 885 Latex offers properties not available in standard styrene-butadiene latexes. FOUNDATIONS 885 Latex is a high solids, low VOC acrylic latex that provides outstanding wet.. |
|||
Glass Transition Temp, Tg | 6.00 °C | 42.8 °F | |
Dow Latex LXC 803F NA Carboxylated Styrene-Butadiene Latex Applications: Latex LXC 803F NA Latex for carpet is an extremely versatile polymer with proven application success in residential, commercial, and unitary carpet backings. The polymer composition of.. |