Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | 41.0 °C | 106 °F | ASTM E1545-00 |
DSM Somos® WaterClear® 10110 Epoxy Resin for Stereolithography
(discontinued **) DescriptionDSM Somos® 10110 is a high-speed liquid photopolymer that produces strong, rigid, and durable parts with optical clarity using stereolithography machines. This material is especially us.. |
|||
Glass Transition Temp, Tg | 41.0 °C | 106 °F | |
Lucite International Elvacite ® 2014 Acrylic Resin Elvacite® 2014 is a medium molecular weight methyl methacrylate copolymer. 2014 is the softest and most flexible of the Elvacite® copolymer grades. It provides good pigment wetting. ElvaciteÂ.. |
|||
Glass Transition Temp, Tg | 41.0 °C | 106 °F | |
Styron DL 242NA Functionalized SB Performance Features: Glass fiber sizing, reactive with external cross-linkersApplications: Fiber Binding, Glass Fiber Binding, Nonwovens and Thermo MoldableLatin America/South AmericaInformation pr.. |
|||
Glass Transition Temp, Tg | 41.0 - 43.0 °C | 106 - 109 °F | ASTM E1545-00 |
DSM Somos® GP Plus 14122 Somos® GP Plus 14122 is a low-viscosity stereolithography resin with an opaque white appearance. This material mirrors production plastics like ABS and PBT, making it an ideal choice for virtually .. |
|||
Glass Transition Temp, Tg | 41.0 °C | 106 °F | dynamic; DIN 53 736 |
Hippe PA 12 Nylon 12 Maintenance-free bearing and gear components under water, insulated components, seals, gear wheels. Parts for pumps and household units. Application in the electrical sector - less water absorptio.. |
|||
Glass Transition Temp, Tg | 41.0 °C | 106 °F | |
3M Scotch-Weld™ DP605NS Structural Adhesive 3M™ Scotch-Weld™ Urethane Adhesives are two-part, non-sag urethane adhesives. They feature tough, flexible bonds with good adhesion to a wide variety of substrates especially wood and many properl.. |