Polymer Property : Glass Transition Temp, Tg = 36.0 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 36.0 °C
96.8 °F
Lucite International Elvacite ® 2550 Acrylic Resin
Elvacite® 2550 is a solid bead methacrylate copolymer resin. It is designed to provide excellent adhesion to metal surfaces and is a resin with good flexibility and medium molecular weight. As su..
Glass Transition Temp, Tg 36.0 °C
96.8 °F
Ultimate Tg
Tra-Con Tra-Bond 293-21 General Purpose Epoxy Adhesive
TRA-BOND 293-21 general purpose epoxy adhesive is designed to provide strong, resilient bonds to a variety of difficult-to-bond substrates, such as gold, nickel, silver, copper, and brass. The 293 s..
Glass Transition Temp, Tg 36.0 °C
96.8 °F
ETM 300-90
ExxonMobil ESCOREZ™ 5380 Petroleum Hydrocarbon Resin
The Escorez 5300 series resins are water white cycloaliphatic hydrocarbon resins. They are designed to tackify a variety of adhesive polymers including EVA, SIS and SEBS block copolymers, metallocen..
Glass Transition Temp, Tg 36.0 °C
96.8 °F
TM R050-25
Resinlab® EP1296 Highly Filled, Moderately Thixotropic Black Casting Resin
Resinlab™ EP1296 is a highly filled, moderately thixotropic black casting resin designed for applications requiring good thermal conductivity, low shrinkage and a low CTE. It was especially formula..