Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | 35.0 °C | 95.0 °F | TM R050-25 |
Resinlab® EP1121-4 Adhesive / Casting Resin Resinlab™ EP1121-4 is a highly filled, high viscosity black adhesive / casting resin designed for applications requiring a high degree of thermal conductivity, flexibility, and a low CTE. It gives .. |
|||
Glass Transition Temp, Tg | 35.0 - 37.0 °C | 95.0 - 98.6 °F | DMA, E |
Proto3000 Objet DurusWhite FullCure430 Polypropylene-like Prototyping Polymer Objet’s FullCure® Materials family of proprietary acrylic-based photopolymer materials enables Objet users to create highly accurate, finely detailed 3D models and parts for a wide range of Rapid .. |
|||
Glass Transition Temp, Tg | 35.0 °C | 95.0 °F | |
Polynorbornene Rubber (PNR) High glass temperature - plasticizer needed to make a 'rubbery' compound. |
|||
Glass Transition Temp, Tg | 35.0 °C | 95.0 °F | |
Mallard Creek Polymers ROVENE® 6017 Styrene-Acrylic Emulsion ROVENE® 6017 is a stiff, self-crosslinking styrene-acrylic copolymer emulsion with excellent water resistance and good mechanical stability.APPLICATIONS: ROVENE® 6017 is recommended for bondin.. |
|||
Glass Transition Temp, Tg | 35.0 °C | 95.0 °F | |
Lucite International Elvacite ® 2046 Acrylic Resin Elvacite® 2046 is a high molecular weight iso-butyl / n-butyl methacrylate copolymer. Elvacite® 2046 is useful in aluminum finishes, ceramic coatings, and aerosol snows. It is soluble in miner.. |
|||
Glass Transition Temp, Tg | >= 35.0 °C | >= 95.0 °F | Dynamic Cure 20—200°C /ISO 25 Min; Ramp 10—200°C @ 20°C/Min |
Epoxy Technology EPO-TEK® 305 Spectrally Transparent Epoxy Product Description: EPO-TEK® 305 is a two component, semi-rigid, optical grade epoxy for semiconductor packaging of fiber optics, optoelectronics and medical devices. It is an electrically and th.. |
|||
Glass Transition Temp, Tg | 35.0 °C | 95.0 °F | |
Asahi Glass Lumiflon LF-302 Solvent Soluble Fluoropolymer w/ Melamine hardening agent Lumiflon was developed by Asahi Glass in 1982, and is unique being the first solvent soluble fluoropolymer. The FEVE based Lumiflon has a alternative copolymer. The complete inter-changeability betw.. |
|||
Glass Transition Temp, Tg | 35.0 °C | 95.0 °F | |
Unitika elitel UE3500 Polyester, Flake High molecular weight, High toughness, High strength, High elongationUNITIKA l resins are thermoplastic saturated copolymeric polyester resins. l resins are expanding their applications from produc.. |