Thermal Properties Metric English Comments
Glass Transition Temp, Tg 343 °C
649 °F
DIN 53 736
Ensinger Tecapeek® Classix Polyaryletherketone (PAEK)
TECAPEEK™ high performance polymer has successfully replaced glass, stainless steel and titanium in a growing range of medical applications. The material's exceptional combination of properties al..