Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | 160 °C | 320 °F | DMA (Tan d Peak); IPC-TM-650.2.4.24.3 |
Park Electrochemical Nelco® N4000-7 SI® FR-4 Epoxy Laminate and Prepreg The Nelco® N4000-7 low-CTE epoxy laminate and prepreg system is a cost-effective solution for use in a broad range of multilayer PCB designs requiring low Z-axis expansion, excellent thermal stabil.. |
|||
Glass Transition Temp, Tg | 160 °C | 320 °F | DMA, ASTM D4065 |
Quantum Composites QC-8560 60% Glass Fiber Vinyl Ester SMC QC-8560 is a vinyl ester based sheet molding compound (SMC) designed for compression molding of components requiring high structural strength. It maintains excellent mechanical properties at temper.. |
|||
Glass Transition Temp, Tg | 160 °C | 320 °F | DSC |
Performance Polymers IPS II PPL-C4150 PEKK (Polyetherketoneketone) Linear 30 % Glass Fiber Reinforced Molding Grade Amber pelletsInformation provided by Infinite Polymer System II. |
|||
Glass Transition Temp, Tg | 160 °C | 320 °F | DSC |
Performance Polymers IPS II PPL-C4219 PEKK (Polyetherketoneketone) Linear Wear Grade Black pellets; Carbon fiber/PTFE/Graphite compoundInformation provided by Infinite Polymer System II. |
|||
Glass Transition Temp, Tg | 160 °C | 320 °F | DSC |
Performance Polymers IPS II PPL-C4250 PEKK (Polyetherketoneketone) Linear 30% Carbon Fiber Reinforced Molding Grade Black pelletsInformation provided by Infinite Polymer System II. |
|||
Glass Transition Temp, Tg | 160 °C | 320 °F | DSC |
Performance Polymers IPS II PPL-C4270 PEKK (Polyetherketoneketone) Linear 40% Carbon Fiber Reinforced Molding Grade Black pelletsInformation provided by Infinite Polymer System II. |
|||
Glass Transition Temp, Tg | 160 °C | 320 °F | Average value: 160 °C Grade Count:4 |
Overview of materials for PEKK, Reinforced This property data is a summary of similar materials in the MatWeb database for the category "PEKK, Reinforced". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
Glass Transition Temp, Tg | 160 °C | 320 °F | DMA (Tan d Peak); IPC-TM-650.2.4.24.3 |
Park Electrochemical Nelco® N4000-7 FR-4 Epoxy Laminate and Prepreg The Nelco® N4000-7 low-CTE epoxy laminate and prepreg system is a cost-effective solution for use in a broad range of multilayer PCB designs requiring low Z-axis expansion, excellent thermal stabil.. |
|||
Glass Transition Temp, Tg | 160 °C | 320 °F | Midpoint; ISO 11357 |
Victrex® HT™ P22 Polyetherketone Product Description: High performance thermoplastic material, unreinforced PolyEtherKetone (PEK), semi crystalline, coarse powder for extrusion compounding, easy flow, FDA food contact compliantInfo.. |
|||
Glass Transition Temp, Tg | 160 °C | 320 °F | Midpoint; ISO 11357 |
Victrex® HT™ P22PF Polyetherketone Product Description: High performance thermoplastic material, unreinforced PolyEtherKetone (PEK), semi crystalline, fine powder for compression compounding, easy flow, FDA food contact compliantInfo.. |
|||
Glass Transition Temp, Tg | 160 °C | 320 °F | Midpoint |
Victrex® HT™ P45 Polyetherketone Product Description: High performance thermoplastic material, unreinforced PolyEtherKetone (PEK), semi crystalline, coarse powder for extrusion
compounding, low flow, FDA food contact compliant, co.. |
|||
Glass Transition Temp, Tg | 160 °C | 320 °F | Midpoint; ISO 11357 |
Victrex® PEEK -HT™ 22GL30 Polyetherketone, 30% Glass Fiber Reinforced Product Description:High performance thermoplastic material, 30% glass fibre reinforced PolyEtherKetone (PEK), semi crystalline, granules for injection moulding, standard flow, FDA food contact comp.. |
|||
Glass Transition Temp, Tg | 160 °C | 320 °F | Midpoint; ISO 11357 |
Victrex® PEEK -HT™ G22 PolyEtherKetone, Unreinforced Product Description:High performance thermoplastic material, unreinforced PolyEtherKetone (PEK), semi crystalline, depth filtered granules for injection moulding, easy flow, FDA food contact complia.. |
|||
Glass Transition Temp, Tg | 160 °C | 320 °F | DSC |
Solvay Specialty Polymers AvaSpire® AV-621 CF30 Polyaryletherketone (PAEK), 30% Carbon Fiber AvaSpire® AV-621 CF30 is a 30% carbon fiber reinforced version of AvaSpire® AV-621. It offers better dimensional stability and warp resistance than 30% carbon fiber reinforced PEEK. The AV-621.. |
|||
Glass Transition Temp, Tg | 160 °C | 320 °F | |
Cosmic Plastics E4940 Mineral & Glass Filled Epoxy Molding Compound, Encapsulated Grade Data provided by the manufacturer. |
|||
Glass Transition Temp, Tg | 160 °C | 320 °F | |
Polyplastics TOPAS® 6015 Cyclic Olefin Copolymer (COC) (Asia/Pacific Grade) A similar grade to 6013. However, heat deflection temperature is (HDT/B) = 150°C. This is a temperature that cannot be achieved with many other amorphous polymers.Information provided by PolyPlasti.. |
|||
Glass Transition Temp, Tg | 160 °C | 320 °F | DSC |
Performance Polymers IPS II PPL-C1050 PEKK (Polyetherketoneketone) Linear Extrusion Grade Amber pellets; neat resinInformation provided by Infinite Polymer System II. |
|||
Glass Transition Temp, Tg | 160 °C | 320 °F | DSC |
Performance Polymers IPS II PPL-C4050 PEKK (Polyetherketoneketone) Linear Molding Grade Amber pellets; neat resinInformation provided by Infinite Polymer System II. |
|||
Glass Transition Temp, Tg | 160 °C | 320 °F | ASTM D3418 |
Solvay Specialty Polymers AvaSpire® AV-621 CF30 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-621 CF30 is a 30% carbon fiber reinforced version of AvaSpire AV-621. It offers better dimensional stability and warp resistance than 30% carbon fiber reinforced PEEK. The AV-621 CF30 gr.. |
|||
Glass Transition Temp, Tg | 160 °C | 320 °F | Midpoint |
Victrex® HT™ P45PF Polyetherketone Product Description: High performance thermoplastic material, unreinforced PolyEtherKetone (PEK), semi crystalline, fine powder for compression compounding, low flow, FDA food contact compliantInfor.. |