Polymer Property : Glass Transition Temp, Tg = 107 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 107 °C
225 °F
Average value: 107 °C Grade Count:3
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), Transparent, Molded". Each property range of values reported is m..
Glass Transition Temp, Tg 107 °C
225 °F
10°C/min test
Polimeri Europa SINKRAL A22V ABS  (discontinued **)
Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,MG,095-25-09-25 Very high flow grade for fast cycle injection moulding. Particularly recommended for the domestic ..
Glass Transition Temp, Tg 107 °C
225 °F
10°C/min test
Polimeri Europa SINKRAL B813 ABS, Impact Grade  (discontinued **)
Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,MG,095-04-35-15 Injection moulding grade, providing very high impact resistance, even at low temperatures. Used as..
Glass Transition Temp, Tg 107 °C
225 °F
Eastman Tenite 180A-28(HT) Cellulose Acetate  (discontinued **)
28% Plasticized.ISO data as provided by the manufacturer, Eastman Chemical.
Glass Transition Temp, Tg 107 °C
225 °F
Eastman Tenite 264-10 CAB Cellulose Acetate Butyrate  (discontinued **)
10% Plasticized. ISO data as provided by the manufacturer, Eastman Chemical.
Glass Transition Temp, Tg 107 °C
225 °F
ASTM D3418
Kolon DIAMAT® EG
Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl..
Glass Transition Temp, Tg 107 °C
225 °F
ASTM D3418
Styrolution Terlux® 2802 HD MABS
Description: Terlux 2802 HD is a standard injection molding Methyl Methacrulate Acrylonitrile Butadiene Styrene grade for transparent parts.Information provided by STYROLUTION, which is a joint vent..
Glass Transition Temp, Tg 107 °C
225 °F
10 K/min; ISO 11357-1/-3
Styrolution Terlux® 2802 TR MABS
Terlux 2802 TR is a standard injection molding MABS grade for tranparent parts.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS.
Glass Transition Temp, Tg 107 °C
225 °F
10 K/min; ISO 11357-1/-3
Styrolution Terlux® 2812 TR MABS
Terlux 2812 TR is a transparent grade of MABS for injection molding with high flowability.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS.
Glass Transition Temp, Tg 107 °C
225 °F
DMTA
Hexcel® HexPly® 920 125°C Curing Epoxy Matrix
HexPly® 920 is a very tough advanced resin matrix, ideally suited to the single-shot production of honeycomb sandwich structures and the manufacture of solid laminates. It is highly tolerant of a v..
Copyright © lookpolymers.com All Rights Reserved