Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | 102 - 122 °C | 216 - 252 °F | Average value: 110 °C Grade Count:21 |
Overview of materials for Acrylic, General Purpose, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, General Purpose, Molded". Each property range of values reported is minimum and maximum values .. |
|||
Glass Transition Temp, Tg | 102 °C | 216 °F | ASTM D3418 |
Kolon DIAMAT® IH Description: DIAMAT® is a specially formulated high impact grade PMMA resin from KOLON. The acrylic composition results in an excellent balance of impact resistance and high modulus at reasonabl.. |
|||
Glass Transition Temp, Tg | 102 °C | 216 °F | |
Lucite International Elvacite ® 3008 Acrylic Resin Elvacite® 3008 is a medium viscosity, methyl methacrylate based bead resin specially designed for use in plastic and vinyl coatings and inks.Information provided by Lucite International |
|||
Glass Transition Temp, Tg | 102 °C | 216 °F | |
Lucite International Elvacite ® 3010 Acrylic Resin Elvacite® 3010 is a medium viscosity, methyl methacrylate based bead resin specially designed for use in plastic and vinyl coatings and inks.Information provided by Lucite International |
|||
Glass Transition Temp, Tg | 102 °C | 216 °F | JIS K7121 |
Zeon Chemicals Zeonor® 1020R Cyclo Olefin Polymer Zeonor® is a line of thermoplastic polyolefin resin with an excellent combination of optical and electronic properties. These unique Cyclo Olefin Polymer (COP) was developed by Zeon Corporation usi.. |
|||
Glass Transition Temp, Tg | 102 °C | 216 °F | Ultimate Tg |
Tra-Con Tra-Bond 526H02 Information provided by Tra-Con Inc. |
|||
Glass Transition Temp, Tg | 102 °C | 216 °F | Ultimate Tg |
Tra-Con Tra-Bond F112 Fiber Optic Epoxy Adhesive TRA-BOND F112 is a long pot life, impact resistant, fiber-optic adhesive. This two-part, low viscosity epoxy has the distinct advantage of remaining below 3000 cps for a minimum of 40 minutes. This .. |
|||
Glass Transition Temp, Tg | 102 °C | 215 °F | ASTM D4065 |
BCC Products MB 5000 Urethane Tooling Board MB 5000 is an extremely tough, high impact Urethane Plank, that can be used for metal forming as well as nickel plating mandrels. Features: excellent machinability, low dust emission, mostly shavin.. |
|||
Glass Transition Temp, Tg | 102 °C | 216 °F | |
Atom Adhesives AA-BOND F112 Epoxy Adhesive AA-BOND F112 is an impact resistant, fiber-optic adhesive. AA-BOND F112 is two-part, low viscosity epoxy has the distinct advantage of remaining below 3000 cps for a minimum of 40 minutes. AA-BOND F.. |
|||
Glass Transition Temp, Tg | 102 °C | 215 °F | ASTM D4065 |
BCC Products MB 3500 Urethane Fixture Board MB 3500 is an extremely tough, high impact Urethane Plank, that can replace aluminum and other metals for many foundry applications. Features: excellent machinability, low dust emission, mostly sha.. |
|||
Glass Transition Temp, Tg | 102 °C | 216 °F | |
Eastman Tenite 525-10 CAB Cellulose Acetate Butyrate
(discontinued **) 10% Plasticized. ISO data as provided by the manufacturer, Eastman Chemical. |