Glass Transition Temp, Tg -78.0 °C
-108 °F
Glass Transition Temperature (10°C/min); ISO 11357-1/-2
DSM Arnitel® EM402-L Polyether Ester Elastomer (European Grade)  (discontinued **)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
Glass Transition Temp, Tg -78.0 °C
-108 °F
10°C/min; ISO 11357-1/-2
DSM Arnitel® EM400 40 Shore D, Injection or Extrusion Grade Copolyester Elastomer (North America)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
Glass Transition Temp, Tg -78.0 °C
-108 °F
Glass Transition Temperature (10°C/min); ISO 11357-1/-2
DSM Arnitel® EM400 Polyether Ester Elastomer (European and Asian Grade)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..
Glass Transition Temp, Tg -78.0 - -60.0 °C
-108 - -76.0 °F
Average value: -70.0 °C Grade Count:4
Overview of materials for Polyether Ester Elastomer
This property data is a summary of similar materials in the MatWeb database for the category "Polyether Ester Elastomer". Each property range of values reported is minimum and maximum values of appr..
Glass Transition Temp, Tg -78.0 °C
-108 °F
10°C/min; ISO 11357-1/-2
DSM Arnitel® EM402-L Injection Molding; Coating Grade Copolyester Elastomer (North America)  (discontinued **)
Product description: Arnitel® combines the advantages of engineering thermoplastics, being easy to process with excellent mechanical properties, at the same time with the flexibility of rubbers.Arn..