Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | -40.0 °C | -40.0 °F | ASTM D4065 |
Solvay Specialty Polymers Solef® 1015 Polyvinylidene Fluoride (PVDF)
(Unverified Data**) Solef® 1015 PVDF homopolymer has very high viscosity, suitable for membrane manufacturing. It is available exclusively as powder.Information provided by Solvay Specialty Polymers. |
|||
Glass Transition Temp, Tg | -40.0 °C | -40.0 °F | ASTM D4065 |
Solvay Specialty Polymers Solef® 6008 Polyvinylidene Fluoride (PVDF)
(Unverified Data**) Solef® 6008 PVDF homopolymer is a low-viscosity PVDF resin and is typically processed by injection molding.Information provided by Solvay Specialty Polymers. |
|||
Glass Transition Temp, Tg | -40.0 °C | -40.0 °F | ASTM D4065 |
Solvay Specialty Polymers Solef® 6012 Polyvinylidene Fluoride (PVDF)
(Unverified Data**) Solef® 6012 PVDF homopolymer is a high-viscosity PVDF resin and is typically processed by extrusion or compression molding.Information provided by Solvay Specialty Polymers. |
|||
Glass Transition Temp, Tg | -40.0 °C | -40.0 °F | DSC, 10ºC/min; DIN 51.007 |
Lubrizol Advanced Materials PEARLTHANE® 11T85UV Thermoplastic Polyurethane Elastomer PEARLTHANE® 11T85UV is a UV resistant polycaprolactone copolyester based TPU, supplied in form of translucent, colourless or slightly yellowish pellets, featuring adequate hardness with excellent.. |
|||
Glass Transition Temp, Tg | -40.0 °C | -40.0 °F | DSC, 50°F/min; DIN 51.007 |
Lubrizol Advanced Materials Pearlthane® 12T92E Thermoplastic Polyurethane Elastomer PEARLTHANE® 12T92E is a special polyester-based TPU, supplied in form of translucent, colorless pellets, combining hardness with excellent processability and low temperature performance. This gra.. |
|||
Glass Transition Temp, Tg | -40.0 °C | -40.0 °F | ASTM D1329 |
Seals Eastern 5242 Neoprene / Chloroprene General purpose neopreneInformation provided by Seals Eastern, Inc. |
|||
Glass Transition Temp, Tg | -40.0 °C | -40.0 °F | ASTM D1329 |
Seals Eastern 5243 Neoprene / Chloroprene General purpose neopreneInformation provided by Seals Eastern, Inc. |
|||
Glass Transition Temp, Tg | -40.0 °C | -40.0 °F | ASTM D1329 |
Seals Eastern 7282 Neoprene / Chloroprene UL-flame resistant, non-blooming neopreneInformation provided by Seals Eastern, Inc. |
|||
Glass Transition Temp, Tg | -40.0 °C | -40.0 °F | ASTM E1356 |
Solvay Specialty Polymers Solef® 1006 Polyvinylidene Fluoride (PVDF) Solef® 1006 PVDF is a very low viscosity homopolymer resin mainly used in injection molding or in multifilament extrusion.Features: Homopolymer; Low ViscosityUses: General PurposeAdditional Prope.. |
|||
Glass Transition Temp, Tg | -40.0 °C | -40.0 °F | DSC |
Solvay Specialty Polymers Solef® 5130 Polyvinylidene Fluoride (PVDF) Solef® 5130 PVDF is an ultra high viscosity grade that gives the best adhesion ideal for its usage in lithium batteries.Features: Good Adhesion; Ultra High ViscosityUses: Batteries; BinderAdditio.. |
|||
Glass Transition Temp, Tg | -40.0 °C | -40.0 °F | ASTM E1356 |
Solvay Specialty Polymers Solef® 6010 Polyvinylidene Fluoride (PVDF) Solef® 6010 PVDF homopolymer has medium viscosity and is typically processed by extrusion.Features: Homopolymer; Medium ViscosityAdditional Properties: Crystallization Heat - ASTM D3417 54.0 to 6.. |
|||
Glass Transition Temp, Tg | -40.0 °C | -40.0 °F | ASTM E1356 |
Solvay Specialty Polymers Solef® 6012 Polyvinylidene Fluoride (PVDF) Solef® 6012 PVDF homopolymer is a high-viscosity PVDF resin and is typically processed by extrusion or compression molding.Features: High Viscosity; HomopolymerAdditional Properties: Crystallizat.. |
|||
Glass Transition Temp, Tg | -40.0 °C | -40.0 °F | ASTM E1356 |
Solvay Specialty Polymers Solef® 60512 Polyvinylidene Fluoride (PVDF) Solef® 60512 PVDF copolymer has high viscosity of the melt and it is a grade for offshore piping.Features: Copolymer; High ViscosityUses: PipingAdditional Properties: Crystallization Heat - ASTM .. |
|||
Glass Transition Temp, Tg | -40.0 °C | -40.0 °F | |
Wanhua Chemical Wanthane® WHT-8190 Polyether-Based TPU Excellent hydrolytic stability, fungus resistance, low temperature flexibility & UV resistanceInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
Glass Transition Temp, Tg | -40.0 °C | -40.0 °F | |
Wanhua Chemical Wanthane® WHT-8195 Polyether-Based TPU Excellent hydrolytic stability, fungus resistance, low temperature flexibility & UV resistanceInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
Glass Transition Temp, Tg | -40.0 °C | -40.0 °F | |
Wanhua Chemical Wanthane® WHT-A890 Aliphatic TPU Non-yellowish, high tensile strength, good abrasion resistance, excellent hydrolytic stability, fungus resistance, low temperature flexibilityInformation provided by Wanhua Chemical Group Co., Ltd. |
|||
Glass Transition Temp, Tg | -40.0 °C | -40.0 °F | DSC |
Lubrizol ESTANE® 58130 Ester Based Thermoplastic Polyurethane Features: Fast cycling, broad temperature performance, and durabilityUse: Injection Molding.Available in Americas, Europe, Middle East, Africa, India and AsiaInformation provided by Lubrizol |
|||
Glass Transition Temp, Tg | -40.0 °C | -40.0 °F | |
Lubrizol Estane® 2102-80A Thermoplastic Polyurethane Elastomer Formerly PellethaneFeature: Low compression setAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 20.. |
|||
Glass Transition Temp, Tg | -40.0 °C | -40.0 °F | |
Lubrizol Estane® 2103-80AE Thermoplastic Polyurethane Elastomer Formerly PellethaneAvailable in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Pellethane product line from Dow in 2009. |
|||
Glass Transition Temp, Tg | -40.0 °C | -40.0 °F | |
3M Dyneon™ LTFE 6400Z Low Temperature Fluoroelastomer 3M™ Dyneon™ Low Temperature Fluoroelastomers LTFE 6400Z are technically advanced low temperature, peroxide-cured fluoroelastomers, designated as a FKM type 3 elastomer per ASTM D1418. They are des.. |
|||
Glass Transition Temp, Tg | -40.0 - -38.0 °C @Frequency 1.00 Hz |
-40.0 - -36.4 °F @Frequency 1.00 Hz |
DMA |
Arkema Group KYNAR® 740 Black/Red Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion Characteristics: Pigmented. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeability, abrasion resistance; high purityAppli.. |
|||
Glass Transition Temp, Tg | -40.0 - -38.0 °C @Frequency 1.00 Hz |
-40.0 - -36.4 °F @Frequency 1.00 Hz |
DMA |
Arkema Group KYNAR® 740 Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili.. |
|||
Glass Transition Temp, Tg | -40.0 - -38.0 °C @Frequency 1.00 Hz |
-40.0 - -36.4 °F @Frequency 1.00 Hz |
DMA |
Arkema Group KYNAR® 740-02 Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. Flame and smoke suppressant. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mecha.. |
|||
Glass Transition Temp, Tg | -40.0 °C | -40.0 °F | Pellet sample |
BASF Elastollan® 1185A10X Wire & Cable Grade Polyurethane Elastomer Compliant with NSF Standard 61 (Drinking water contact). As with all TPU products this grade must be dried prior to processing.Information provided by BASF Corporation. |
|||
Glass Transition Temp, Tg | -40.0 - -38.0 °C @Frequency 1.00 Hz |
-40.0 - -36.4 °F @Frequency 1.00 Hz |
DMA |
Arkema Group KYNAR® 460 Polyvinylidene Fluoride Homopolymer - Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. Broad molecular weight distribution. High stability in harsh thermal, chemical and ultraviolet environments. High toughness a.. |
|||
Glass Transition Temp, Tg | -40.0 - -38.0 °C @Frequency 1.00 Hz |
-40.0 - -36.4 °F @Frequency 1.00 Hz |
DMA |
Arkema Group KYNAR® 720, 720 HDP Polyvinylidene Fluoride Homopolymer- Injection Molding and Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. HDP indicates higher color stability. High stability in harsh thermal, chemical and ultraviolet environments. High toughness .. |
|||
Glass Transition Temp, Tg | -40.0 °C | -40.0 °F | |
Sorbothane Polyurethane Damping Material, 70 Durometer Sorbothane® is a thermoset, polyether-based polyurethane viscoelastic material that combines high energy absorption with faultless memory. Sorbothane turns mechanical energy into heat. As the mat.. |
|||
Glass Transition Temp, Tg | -40.0 - -38.0 °C @Frequency 1.00 Hz |
-40.0 - -36.4 °F @Frequency 1.00 Hz |
DMA |
Arkema Group KYNAR FLEX® 2850-07 Polyvinylidene Fluoride Copolymer - Extrusion & Molding Characteristics: Natural resin - translucent, off-white hemispheres. 150°C Temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechani.. |