Thermal Properties | Metric | English | Comments |
---|---|---|---|
Glass Transition Temp, Tg | -117 °C | -179 °F | Silicone Property; ASTM D3418 |
Arlon CP-499CA Bulk Compound This data represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Information provided by Arlon, Silicone Technologies Di.. |
|||
Glass Transition Temp, Tg | -117 °C | -179 °F | Arlon SQA-TMS-055 |
Arlon R3781-920-##R##-P0 Silicone Rubber This fusible silicone tape is specially formulated to yield improved flexibility, elongation and elastic recovery at low operating temperature (-70°C to -100°C) where standard fusible silicone tap.. |