Thermal Properties | Metric | English | Comments |
---|---|---|---|
Specific Heat Capacity | 2.60 J/g-°C @Temperature 150 °C |
0.621 BTU/lb-°F @Temperature 302 °F |
DSC |
Total 3802 B HDPE, cable, sheet, pipe, injection molding FINATHENE® 3802 B is a polyethylene copolymer based on C6 hexene as co-monomer and is produced by a continuous low-pressure slurry polymerization process. FINATHENE® 3802 B is a black polyethylene.. |
|||
Specific Heat Capacity | 2.60 J/g-°C @Temperature 150 °C |
0.621 BTU/lb-°F @Temperature 302 °F |
DSC |
Total 3802 Blue MDPE pipe, injection molding FINATHENE® 3802 Blue is a polyethylene copolymer based on C6 hexene as co-monomer and is produced by a continuous low pressure slurry polymerization process. FINATHENE® 3802 Blue is a blue polyeth.. |
|||
Specific Heat Capacity | 2.60 J/g-°C @Temperature 150 °C |
0.621 BTU/lb-°F @Temperature 302 °F |
DSC |
Total 3802 YCF MDPE pipe grade FINATHENE® 3802 Y CF is a polyethylene copolymer based on C6 hexene as co-monomer and is produced by a continuous low pressure slurry polymerization process. FINATHENE® 3802 Y CF is a yellow cadmi.. |
|||
Specific Heat Capacity | 2.60 J/g-°C @Temperature 150 °C |
0.621 BTU/lb-°F @Temperature 302 °F |
DSC |
Total HP 401 MDPE, pipe, cable, sheet FINATHENE® HP 401 is a polyethylene copolymer based on C6 hexene as co-monomer and is produced by a continuous low-pressure slurry polymerization process. FINATHENE® HP 401 is a black high densit.. |
|||
Specific Heat Capacity | 2.60 J/g-°C @Temperature 150 °C |
0.621 BTU/lb-°F @Temperature 302 °F |
DSC |
Total Xsene® XS10 B HDPE, pipe, injection molding FINATHENE® XS10 B is a high density polyethylene based on C6 hexene as co-monomer and is produced by the Fina Double Loop Technology™. FINATHENE® XS10 B is a high performance black compound speci.. |
|||
Specific Heat Capacity | 2.60 J/g-°C @Temperature 150 °C |
0.621 BTU/lb-°F @Temperature 302 °F |
DSC |
Total Xsene® XS10 H HDPE, pipe, injection molding FINATHENE® XS 10 H is a high density polyethylene based on C6 hexene as co-monomer and is produced by the Fina Double Loop Technology™. FINATHENE® XS 10 H is a high performance dark blue compound.. |
|||
Specific Heat Capacity | 2.60 J/g-°C | 0.621 BTU/lb-°F | |
DuPont Performance Polymers Zytel® FG408L NC010 Nylon 66
(Unverified Data**) Unreinforced Toughened Polyamide 66 with Developed for Food Contact Applications Zytel FG408L NC010 is a general purpose lubricated impact modified polyamide 66 resin with superior toughness for inj.. |
|||
Specific Heat Capacity | 2.60 J/g-°C @Temperature 150 °C |
0.621 BTU/lb-°F @Temperature 302 °F |
DSC |
Total Lacqtene® 2001 TBK 46 HDPE pipe
(discontinued **) LACQTENE® 2001 TBK 46 is a high density polyethylene produced by the gas phase polymerization process. LACQTENE® 2001 TBK 46 is a black compound especially developed for pressure pipe for gas and .. |
|||
Specific Heat Capacity | 2.60 - 2.60 J/g-°C @Temperature 150 - 150 °C |
0.621 - 0.621 BTU/lb-°F @Temperature 302 - 302 °F |
Average value: 2.60 J/g-°C Grade Count:8 |
Overview of materials for High Density Polyethylene (HDPE), Pipe Grade This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Pipe Grade". Each property range of values reported is minimum and max.. |
|||
Specific Heat Capacity | 2.60 J/g-°C @Temperature 150 °C |
0.621 BTU/lb-°F @Temperature 302 °F |
DSC |
Total Xsene® XS10 Orange YCF HDPE, pipe FINATHENE® XS 10 ORANGE YCF is a high density polyethylene based on C6 hexene as co-monomer and is produced by the Fina Double Loop Technology™. FINATHENE® XS 10 ORANGE YCF is a high performance .. |